Excellent resistance to oxidation, sulfidation, and carburization
• Higher creep and rupture properties for high temperature situations above 1100°F (600°C)
• Resistant to high temperature corrosion and prolonged exposure
• Readily machined by standard methods
• Resistance to aqueous corrosion at moderate temperatures
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 800ht in China. If you're going to wholesale high quality inconel 800ht made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Super alloys are also referred to as high performance alloys. They have good creep and oxidation resistance, and are utilized where high surface stability is required. They also have an ability to function under high temperatures and mechanical stress. They can be strengthened by solid-solution hardening, work hardening, and precipitation hardening. They are divided into three groups such as iron-based, nickel-based, and cobalt-based alloys.

 

Incoloy 800HT is a nickel-iron-chromium alloy, and also a modified version of alloy 800. It has high creep-rupture strength. The following datasheet gives an overview of Incoloy 800HT.

 

Product Parameter
 

 

PRODUCT FORM

SIZE RANGE FROM

SIZE RANGE TO

Alloy 800HT pipe

0.5 in

8 in

Alloy 800HT tube

12 mm

260 mm

Alloy 800HT pipe fittings

0.5 in

8 in

Alloy 800HT flanges

0.5 in

8 in

 

Feature
 
product-78-78

CHEMICAL COMPOSITION

The base composition of 800H/HT is identical to the parent Alloy 800. However, in both 800H® and 800HT, the levels of carbon, aluminum, and titanium are modified for improved creep resistance. The base 800 grade has a carbon range of 0 - 0.10%, while 800H raises the minimum carbon level to 0.05%. Similarly, the base 800 grade has a combined aluminum and titanium content requirement of 0.30 - 1.20%, while 800HT raises the minimum Al + Ti level to 0.85% and increases the minimum carbon to 0.06%.

 
product-78-78

CORROSION RESISTANCE

Both grades share the corrosion resistant characteristics of the base grade Alloy 800, including good general corrosion resistance, as well as good resistance to reducing and oxidizing acids, organic acids, seawater, salts, and particularly excellent resistance to nitric acid. Alloy 800H and 800HT also exhibit excellent corrosion resistance to chloride stress corrosion cracking (SCC). However, alloys 800H and 800HT are not recommended for sulfuric acid service. Additionally, they are susceptible to chromium carbide precipitation along grain boundaries when subjected to temperatures in the range of 1000°F - 1400°F (538°C - 760°C).

 
product-78-78

ELEVATED TEMPERATURE RESISTANCE

800H and 800HT have outstanding resistance to oxidation, carburization, and sulfidation at temperatures up to 1800°F.

 
product-78-78

MECHANICAL PROPERTIES

800H and 800HT are typically supplied in a low-strength solution annealed condition. While intended for high-temperature applications, they have excellent toughness down to cryogenic temperatures.

 
product-78-78

HEAT TREATMENT

Alloys 800H and 800 HT cannot be strengthened by heat treating. They are typically solution annealed at 2050°F - 2150°F (1121°C - 1177°C) followed by rapid cooling. Stress-relieving at 1000°F - 1600°F (538°C - 870°C) may also be performed after cold working to reduce residual stresses and prevent distortion.

 
product-78-78

WORKABILITY

Alloy 800H and 800HT can be cold worked using common methods and should be in the annealed condition prior to cold working. The large grain size produced in both grades from solution annealing can lead to “orange peel” surface roughening after cold working. Hot-working should be done above 1600°F (871°C).

 

 

Application
 

 

Alloy 800H and 800HT are used at temperatures from 1100°F – 1800°F (593°C – 982°C) where creep and stress rupture failure is a concern. 800H® is typically used at the lower end of this range, while 800HT is employed at the upper end. Applications include structural members, furnace equipment, heat exchangers, petrochemical vessels and piping, and aerospace. CRA offers specialty alloy 800H/HT seamless pipe & tube for use in multiple industries and applications, including:
• Furnace Equipment
• Aerospace
• Petrochemical Vessels & Piping
 

Our Company
 

 

product-750-416

38000㎡ workshop and 200+ emplovees to meet your huge demands.

 

Packing & Delivery
 

 

product-750-750

 

Our nickel based bars are packaged professionally to ensure they remain intact during transportation and storage. Our packaging materials have been carefully selected to protect nickel based bars from moisture, pollution, and damage. We can provide different packaging methods according to your requirements, such as wooden boxes, pallets, cardboard boxes, etc., to meet your specific needs. Our packaging process strictly follows international standards to ensure that the nickel based bars you receive are high-quality and undamaged products. No matter how much quantity or size you need, we can provide you with efficient, reliable, and satisfactory services. Please contact us for more information.

 

Customer Visit
 

 

product-750-464

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ
 

 

Q: What is your terms of payment ?

A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable.

Q: What are the advantages of your company ?

A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other Nickel base alloy companies.

Q: How many coutries you already exported ?

A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Q: Can you provide sample ?

A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

 

Hot Tags: inconel 800ht, China inconel 800ht suppliers, alloy for high pressure applications, alloy for sealing applications, alloy for fatigue resistance, alloy for chromatography baths, alloy for photonics, alloy materials

Send Inquiry

whatsapp

Phone

E-mail

Inquiry