GH3030 Pipe
video

GH3030 Pipe

GH3030 tubing is widely used in various fields, especially in industries with high-temperature and corrosive environments such as aerospace, chemical, and power generation.

Grade: GH3030
Surface Treatment: 2B, 2D, BA NO(8)
Shape: Round, Square, Rectangular
Type: Seamless/ERW/Welded
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3030 pipe in China. If you're going to wholesale high quality gh3030 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GH3030 Seamless Pipe description

 

GNEE Alloy 3030 Seamless Pipe

GNEE Alloy 3030 Seamless Pipe

 

GH3030 (equivalent to Nimonic 75) tubing is a nickel-chromium-based solid solution-strengthened high-temperature alloy designed specifically for high-temperature structural integrity. Our GH3030 tubing is widely recognized for its excellent oxidation resistance and thermal fatigue strength, with long-term temperature resistance up to 800°C and short-term temperature resistance up to 1000°C.

 

Due to its simple chemical composition and mature manufacturing process, GH3030 tubing perfectly balances cost-effectiveness with high performance and durability. It is ideal for combustion chamber components, heat exchangers, and furnace assemblies.

Need a specific wall thickness or length? We offer custom-cut GH3030 seamless and welded steel pipe with short lead times.

Get a free quote within 24 hours

 

 

High temperature Alloy GH3030 Seamless Pipe Specification

 

Specifications of High Temperature Gh3030 PIPES / TUBE:
Grade High Temperature Gh3030
Range 1/2″ Nominal Bore To 16″Nominal Bore
Length Single Random, Double Random & Cut Length.
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Round, Square, Rectangular, Hydraulic Etc
Type Seamless / ERW / Welded / Fabricated / EFW
Applications Off-Shore Oil Drilling Companies, Power Generation, Petrochemicals, Gas Processing, Specialty Chemicals, Pharmaceuticals, Pharmaceutical Equipment, Chemical Equipment, Sea Water Equipment, Heat Exchangers, Condensers, Pulp and Paper Industry

 

Nimonic 75 Seamless Pipe Specification

 

CHEMICAL COMPOSITION OF High Temperature Gh3030 Pipe
Grade C Mn Si S Ti Fe Ni Cr P Al
GH3030 0.12 max 0.70 max 0.80 max 0.02max 0.15-0.35 1.5max balance 19.00 – 22.00 0.03 0.15

 

GH3030 - UNS GH30 / XH78T High Temperature Alloy Pipe Mechanical Properties

Element Yield Strength (0.2%Offset) Melting Point Density Tensile Strength Elongation
GH3030 MPa – 1420 °C 8.4 g/cm3 MPa – 785 Min 35 %

Click to download the GH3030 alloy PDF file now

 

GH3030 pipe available in a range of sizes (standard and custom sizes)

 

We offer GH3030 tubes in both Seamless (Cold Rolled/Cold Drawn) and Welded versions to suit different pressure and cost requirements.

Type Outside Diameter (OD) Wall Thickness (WT) Length
Seamless Tube 6mm – 219mm 0.5mm – 20mm Up to 12,000mm
Welded Pipe 10mm – 508mm 1.0mm – 15mm Up to 12,000mm
Capillary Tube 0.5mm – 6.0mm 0.1mm – 1.0mm Coil or Straight

 

GH3030 High Temperature Alloy Tube: Size Chart and Pressure Ratings

 

As experts in high temperature alloys, Gnee Steel understands that precision and safety are paramount. Below is a technical reference table for our GH3030 (nickel-chromium alloy) seamless tubes.

 

1. GH3030 Common Size Chart (Standard Sizes and Stock Sizes)

We maintain ample stock of standard sizes and offer custom machining services for non-standard sizes.

Outside Diameter (OD) Wall Thickness (WT) Type Theoretical Weight ( kg/m )
6.0 mm 0.5 mm / 1.0 mm Seamless / Capillary 0.069 / 0.126
10.0 mm 1.0 mm / 1.5 mm Seamless 0.227 / 0.321
18.0 mm 1.5 mm / 2.0 mm Seamless 0.623 / 0.806
25.0 mm 2.0 mm / 3.0 mm Seamless 1.159 / 1.663
38.0 mm 2.5 mm / 4.0 mm Seamless 2.235 / 3.427
57.0 mm 3.0 mm / 5.0 mm Seamless 4.080 / 6.552
76.0 mm 4.0 mm / 6.0 mm Seamless 7.252 / 10.584
108.0 mm 5.0 mm / 8.0 mm Seamless / Welded 12.978 / 20.160
219.0 mm 6.0 mm / 10.0 mm Welded / Forged 32.128 / 52.668

Note: Custom outer diameters (maximum 508 mm) and wall thicknesses are available upon request. Lengths are available in random or fixed sizes, up to 12 meters.

 

2. Pressure Rating Table for GH3030 Pipes

The rated pressure of GH3030 varies significantly with operating temperature. The following values ​​are calculated based on the Barlow formula (P = 2St/D) and use a standard safety factor.

OD x WT (mm) at 20°C (MPa) at 600°C (MPa) at 800°C (MPa)
10 x 1.0 24.5 MPa 18.2 MPa 8.5 MPa
18 x 1.5 20.4 MPa 15.1 MPa 7.1 MPa
25 x 2.0 19.6 MPa 14.5 MPa 6.8 MPa
38 x 3.0 19.3 MPa 14.3 MPa 6.7 MPa
57 x 4.0 17.2 MPa 12.7 MPa 5.9 MPa
76 x 5.0 16.1 MPa 11.9 MPa 5.6 MPa
108 x 8.0 18.1 MPa 13.4 MPa 6.3 MPa

GH3030 tubing exhibits excellent structural stability. However, as shown above, its permissible pressure decreases by approximately 60-70% when the temperature rises from room temperature to 800°C. This is particularly relevant for ultra-high pressure applications above 800°C.

Click to contact us for customized pipe size solutions

 

GH3030 Pipe Manufacturing Process

 

Quality stems from exquisite craftsmanship. Our GH3030 pipes undergo a rigorous multi-stage production process:

Vacuum Melting/ESR: Ensures ultra-pure material with extremely low impurity content.

Hot Extrusion: Forms a seamless hollow tube body.

Multi-pass Cold Rolling/Drawing: Achieves precise dimensional accuracy and superior surface finish.

Bright Annealing (Solution Treatment): Rapid cooling at 1100°C to 1150°C restores ductility and corrosion resistance.

Non-destructive Testing: 100% eddy current and ultrasonic testing ensures zero-defect integrity.

Vacuum melting/ESR
Vacuum melting/ESR
Bright Annealing
Bright Annealing
100% Eddy Current Testing
100% Eddy Current Testing
Ultrasonic Testing
Ultrasonic Testing

 

The delivery time for GH3030 Seamless Pipe varies depending on the location

 

Cost Changes 5 % extra
Export to Delivery Time
UAE 5 days
Qatar 7
France 30
Kuwait 10
USA 40-60
Saudi Arabia 7
Oman 5
Italy 30
Uk 30

 

Products and services offered by Gnee Steel

 

Main Applications of GH3030 Steel Pipe

 

GH3030 steel pipe is a key component in industries where high-temperature and oxidizing environments are critical:

Aerospace and Defense: Jet engine combustion chamber fuel lines, fuel manifolds, and afterburner guide vanes.

Industrial Furnaces: Radiant tubes, muffle furnaces, thermocouples, and heat treatment furnaces.

Petrochemical and Energy: Corrosive high-temperature gas heat exchangers and catalyst support tubes.

Automotive: High-performance exhaust system components and sensor housings.

Main Applications of GH3030 Steel Pipe

Combustion chamber fuel lines
Combustion chamber fuel lines
product-1000-722
Radiant heating pipes
product-1000-560
Petrochemical components
product-810-535

Automotive exhaust components

 

 

Packaging method for Alloy 400 Pipe

Packaging method for Alloy 400 Pipe

 

Gnee Steel uses the safest and most effective packaging methods for all types of cargo transportation. Our packaging methods include:

Wooden crates
Wooden pallets
Shrink wrap packaging
Cardboard boxes
Wooden crates (slatted)

Every GH3030 pipe we ship comes with a certified EN 10204 3.1 Material Testing Certificate (MTC), which includes chemical, mechanical, and non-destructive testing reports.

View our quality certificates

 

About Gnee Steel

 

About Gnee Steel

 

About Gnee Steel

Request the latest High Temperature Alloy GH3030 Pipe price list. Please call +8615824687445 or email ss@gneesteel.com for information on available stock and the latest price list for Nickel GH3030 Pipe.

modular-1
Please contact us to get a quick quote for the Alloy GH3030 Pipe you need

We supply these GH3030 Pipe and tubes according to DIN, ISO, JIS, or ANSI/ASME standards.

FAQ

 

Q1: Can GH3030 tubes be easily welded?
A: Yes. GH3030 has excellent weldability. It can be welded using Argon Arc Welding (TIG), Plasma Welding, or Resistance Welding. We recommend using matching GH3030 filler wire to ensure the weld seam maintains the same oxidation resistance as the base metal.

 

Q2: What is the maximum continuous working temperature?
A: For long-term load-bearing applications, we recommend a limit of 800°C. For non-load-bearing oxidation resistance (e.g., sensor guards), it can withstand up to 1000°C.

 

Q3: Is GH3030 suitable for high-pressure environments?
A: Our seamless GH3030 tubes are designed for high-pressure applications. We perform hydrostatic testing on every pipe to ensure it meets your specific pressure safety requirements.

 

Q4: Do you offer samples for testing?
A: Yes, we can provide small-batch samples for material verification and welding trials. Please contact our sales team for availability.

Hot Tags: gh3030 pipe, China gh3030 pipe suppliers, Casting High Temperature Alloy