GH4141 High Temperature Alloys Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4141 high temperature alloys pipe in China. If you're going to wholesale high quality gh4141 high temperature alloys pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH4141 High Temperature Alloys Pipe
1. Manufacturing springs and bolts that work at high temperatures; rotor blades, impellers and other structural parts on gas turbines;
2. The thrust chamber on the rocket engine;
3. Thrust reverse device on the aircraft;
4. Large high-pressure vessel;
5. Elastic air sealing sheet, elastic sealing die sheet, rubber mechanical electric heating blade.
GH4141 is a Ni-Cr-Co-based precipitation hardening deformed superalloy, which mainly relies on aging precipitation of γ' phase and M, C type carbides for strengthening. This alloy can be used below 980°C and exhibits extremely high tensile, durability and creep strength in the range of 650°C to 900°C. Yield resistance and fatigue resistance, as well as good oxidation resistance, make GH4141 one of the plate alloys with the highest mechanical properties when used below 980°C. Its good machinability means it is suitable for applications in a variety of high-temperature environments, such as turbine disks, guide vanes, combustion chamber plate load-bearing parts, turbine rotors, guides, fasteners and high-temperature springs in aviation and aerospace engines and other parts.