GH3128 High Temperature Resistant Metal Plate
video

GH3128 High Temperature Resistant Metal Plate

1.Product Name: High Temperature Alloy Plate/Sheet
2.Grade: GH3128
3.Thickness: 0.6mm-70mm, Length: ≤12000mm, Wide:≤2500mm
4.Features: High temperature alloy (GH3128), solid solution strengthened nickel-based alloy, it has good overall performance with high durable, also with high plasticity, high persistent creep strength, good oxidation resistance and stamping, welding and other performance.
5.Applications:
aircraft engine combustion chamber flame cylinder, afterburner shell and regulating plate.
Structure of gas turbine combustion chamber.
Turbine engine combustion chamber components.
Afterburner parts.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3128 high temperature resistant metal plate in China. If you're going to wholesale high quality gh3128 high temperature resistant metal plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GNEE GH3128 high temperature resistant metal plate introduce

GH3128 high temperature metal plate

GH3128 nickel-based alloy plate is a high-temperature nickel-chromium alloy strengthened with tungsten and molybdenum, known for its excellent oxidation resistance and strength up to 950°C. Produced by a specialist mill in China, this alloy is designed for extreme environments. Whether you need GH3128 nickel alloy plate, GH3128 nickel alloy sheet and plate or GH3128 plate, it delivers top performance in critical applications.

GNEE GH3128 plate Specification

GH3128 metal plate

GH3128 high temperature resistant metal plateGH3128 high temperature resistant metal plate

Our GH3128 high temperature resistant metal plates come in a variety of configurations:

Thickness: 0.5mm to 50mm
Width: up to 1500mm
Length: up to 6000mm or cut to size
Surface treatment: polished, brushed or calendered
Standard: GB/T 14992
Need a specific nickel-based alloy plate specification? We at Gnee Steel offer tailor-made solutions!

GNEE GH3128 high temperature plate Application

GH3128 resistant metal plate

GH3128 high temperature resistant metal plateGH3128 high temperature resistant metal plate

Applications

The GH3128 Alloy Plate serves high-temperature industries:

Aerospace: Turbine blades and combustor components.

Power Generation: Boiler parts and heat exchangers with GH3128 Nickel Alloy Plate Rolling.

Chemical Processing: Liners like GH3128 Nickel Alloy Sheets and Plates in oxidizing systems.

Industrial Furnaces: Structural components in extreme heat.

Gas Turbines: High-temperature GH3128 Plate for engine parts.

GNEE GH3128 high temperature resistant metal plate Sizes and Specifications 

Common sizes of GH3128 plates:

Category Thickness Range Width Range Length Range Example Dimensions
Thin Plate 0.5 mm - 3.0 mm 600 mm - 1500 mm 1000 mm - 6000 mm 1.0 mm × 1000 mm × 2000 mm
Medium Plate 3.0 mm - 20.0 mm 600 mm - 1500 mm 1000 mm - 6000 mm 10.0 mm × 1200 mm × 2400 mm
Thick Plate 20.0 mm - 50.0 mm 600 mm - 1500 mm 1000 mm - 6000 mm 25.0 mm × 1500 mm × 3000 mm
Custom Sizes Customizable as needed Customizable as needed Customizable as needed Non-standard thickness, width, length

Notes:

Thickness: Divided into thin, medium, and thick plates, ranging from 0.5 mm to 50.0 mm.

Width: Common widths range from 600 mm to 1500 mm, with customizable options for special requirements.

Length: Common lengths range from 1000 mm to 6000 mm, with customizable options for special requirements.

Example Dimensions: Lists some typical standard dimensions for reference.

GNEE Group Factory Environment 

GNEE Group  Factory Environment

GH3128 high temperature resistant metal plate

GNEE Group Product Delivery

GNEE Group Product Delivery

GH3128 high temperature resistant metal plate

FAQ

Q: What's the terms of packing?
A: Generally,we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q: What's your delivery time?
A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit.
Q: Could you produce according to the samples?
A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.

Hot Tags: gh3128 high temperature resistant metal plate, China gh3128 high temperature resistant metal plate suppliers, Casting High Temperature Alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry