GH4141 4145 High Temperature Ss Alloys Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4141 4145 high temperature ss alloys pipe in China. If you're going to wholesale high quality gh4141 4145 high temperature ss alloys pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH4141 4145 High Temperature Ss Alloys Pipe Products Description
GH4141 4145 high temp alloys Pipe video
GNEE STEEL GROUP supplies GH4141 4145 High Temperature Ss Alloys Pipe for you
| Category | Type | Grade | Designations |
|---|---|---|---|
| Grades | Superalloys | GH4141 | China - GB , |
| Category | Type | Grade | Designations |
|---|---|---|---|
| Grades | Superalloys | GH4145 | China - GB , |
GH4141 4145 High Temperature Ss Alloys Pipe chemical composition
GH4141 High Temperature Ss Alloys Pipe chemical composition
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
|---|---|---|---|---|
| C | 0.06 | 0.12 | ||
| Cr | 18.0 | 20.0 | ||
| Mo | 9.0 | 10.5 | ||
| Ni | - | Remainder | ||
| Co | 10.0 | 12.0 | ||
| Al | 1.4 | 2.0 | ||
| Nb | 2.5 | 3.9 | ||
| Ti | 2.9 | 3.5 | ||
| B | 0.003 | 0.01 | ||
| Fe | - | 0.5 |
GH4145 Superalloy alloy chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
Nb |
Co |
C |
Mn |
Si |
S |
Cu |
Al |
Ti |
|
GH4145 |
Min |
14 |
5.0 |
0.7 |
0.4 |
2.25 |
|||||||
|
Max |
70 |
17 |
9.0 |
1.2 |
1.00 |
0.08 |
1.00 |
0.50 |
0.01 |
0.5 |
1.0 |
2.75 |
GH4141 4145 high temperature ss alloys Pipe


GH141 is a precipitation hardening nickel-based deformed high-temperature alloy with high tensile and durable creep strength and good oxidation resistance in the range of 650 to 950°C. Due to the high content of aluminum, titanium and molybdenum in the alloy, it is difficult to open the ingot. However, the deformed material has good plasticity and can be cold formed in the annealed state and can also be welded. Strain is easily generated during heat treatment of welded parts. Age cracks.This alloy is mainly used to manufacture ring parts, structural parts, bolts and other parts of aero engines that work below 800°C and require high strength and corrosion resistance, and planes that have medium or low stress and require relaxation resistance that work below 540°C. Springs and coil springs. It can also be used to manufacture parts such as turbine blades.
Product technology


Product packaging

Customer Case
customer visit

FAQ
Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.
Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable
Q: About the product price of GH4141 4145 high temperature metal alloys Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: gh4141 4145 high temperature ss alloys pipe, China gh4141 4145 high temperature ss alloys pipe suppliers, Casting High Temperature Alloy
You Might Also Like
Send Inquiry