Super Invar 32-5 BAR
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super invar 32-5 bar in China. If you're going to wholesale high quality super invar 32-5 bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Super Invar 32-5, a magnetic, austenitic, solid solution alloy containing iron, nickel and cobalt, is designed to provide minimum thermal expansion at room temperatures. This alloy also exhibits austenite stability to service temperatures at least -67°F (-55°C) and thermal expansion properties less than those of Invar 36 alloy (36% nickel-iron) when used in the-67/203°F (-55/95°C) temperature range.l
Super Invar is manufactured to provide minimum thermal expansion at room temperatures. The thermal expansion rates exhibited by this alloy is less than half of Invar 36 with a narrower application temperature range due to a lower Curie temperature. The alloy exhibits austenite stability to service temperatures at least -67°F (-55°C). ASTM F1684 and UNS K93500 are the specification references.
Although Super Invar has a substantially lower expansivity than Invar, it is susceptible to martensite transformation in the vicinity of -30°C. (-22°F), due to its reduced nickel content.
Super Invar has a very low coefficient of thermal expansion at temperatures from below -50°C. (-58°F.) up to about 100°C. (212°F.). It also exhibits thermal stability, a martensitic transformation inception point which is controlled, so as to fall well below the lowest temperature to be encountered in the particular application.
Common Trade Names:
Invar 32-5 , Nickel 32-5 Alloy , UNS K93500 , 4J32
Super Invar 32-5 Chemical Composition
| C | Si | P | S | Cu | Mn | Co | Ni | Fe |
|---|---|---|---|---|---|---|---|---|
| ≤0.05 | ≤0.2 | ≤0.02 | ≤0.02 | 0.4-0.8 | 0.2-0.6 | 3.2-4.2 | 31.5-33.0 | Balance |
Super Invar 32-5 Physical Properties
| Density | Melting range |
|---|---|
| 8.15 g/cm³ | 1430~1450℃ |
Super Invar 32-5 Alloy Mechanical Properties
| Properties | Tensile strength | Yield strength | Modulus of elasticity | Poisson's ratio | Elongation at break (in 2 in. (50.8 mm)) | Hardness, Rockwell B (annealed) | Hardness, Rockwell B (cold worked) | Machinability |
|---|---|---|---|---|---|---|---|---|
| Metric | 483 MPa | 276 MPa | 145 GPa | 0.23 | 40% | 75 | 90 | 25 |
| Imperial | 70000 psi | 40000 psi | 21000 ksi | 0.23 | 40% | 75 | 90 | 25 |
Fabrication and Heat Treatment:
Machinability
Super alloy Invar 32-5 can be machined using all conventional methods. Slow speeds and positive feeds are preferred for this alloy
Forming
Super alloy Invar 32-5 can be formed using all conventional methods.
Welding
Super alloy Invar 32-5 can be welded using conventional techniques.
Cold Working
Super alloy Invar 32-5 can be cold worked using conventional techniques as it has high ductility.
Annealing
Super alloy Invar 32-5 is annealed at 844°C (1550°F) followed by quenching in water.
Super Invar 32-5 Available Shape
Super Invar 32-5 Size Range
»Round Bar & Square Bar & Hexagon Bar
● Diameter : φ8~φ300mm Length:10mm-6000mm
● Hot forging, Hot Rolling, Cold Drawing
● Bright Surface, Polished Surface, Black Surface
»Tube & Pipe:Seamless Tube& Welded Pipe
● Cold Drawing Seamless Pipe: φ1.0~φ220mm
● Hot Extrusion pipe: φ50~φ250mm
● Others : U Blend Tube and Elbow
»Hot Rolled Plate & Cold Rolled Sheet
● Cold Rolling Sheet Thickness: ≦2.0mm Width:≦1500m
● Hot rolling Plate Thickness: ≧4.0mm Width: ≦2500m
»Strip & Tape Ribbon
● Thickness: ≧ 0.01mm Width: 15mm-300mm
● Cold rolling BA Strip, Hard & Soft Condition
»Straight Length Wire & Spool Wire
● Welding Wire: φ 0.1mm~6.0mm Cut length Rod: φ1.0~φ8.0mm
● Package : 5-25kg/Spool or Box


FAQ
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable
Hot Tags: super invar 32-5 bar, China super invar 32-5 bar suppliers, Casting High Temperature Alloy
Previous
Hiperco 50 Alloy BarYou Might Also Like
Send Inquiry