Hastelloy Alloy S Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy alloy s pipe in China. If you're going to wholesale high quality hastelloy alloy s pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy alloy S pipe is manufactured from Hastelloy alloy S, a nickel-based superalloy that is highly resistant to corrosion and oxidation. This alloy is specifically designed for use in extremely harsh environments, including those with high concentrations of chloride ions and sulfuric acid at elevated temperatures.
Uses of Hastelloy Alloy S Pipe:
Chemical Processing: It is widely used in the chemical processing industry, especially where there is exposure to sulfuric acid and other aggressive chemicals.
Petroleum Refining: In the petroleum industry, it is used in equipment that comes into contact with hydrocarbons and acids during the refining process.
Nuclear Industry: It is also utilized in certain applications within the nuclear industry due to its excellent resistance to high-temperature, corrosive environments.
Marine Applications: Given its resistance to chloride and seawater, it can be used in marine applications as well.
Physical Properties
| Density | g/cm3 | 8.75 | |
|---|---|---|---|
| lb/in.3 | 0.316 | ||
| Melting Range | °F | 2435 - 2516 | |
| °C | 1335 - 1380 | ||
Mechanical Properties
| Form | Aging Temperature | Aging Time | Yield Strength (0.2% Offset) |
Tensile Strength | Elongation | |||
|---|---|---|---|---|---|---|---|---|
| °F | °C | h | ksi | Mpa | ksi | MPa | % | |
| Gas Tungsten arc Welded Plate ½ in (12.7mm) Thick | Solution Heat-treated | - | 59.8 | 412 | 112.4 | 775 | 62 | |
| 1000 | 63.3 | 436 | 121.7 | 839 | 33 | |||
| 4000 | 60.4 | 416 | 122.8 | 847 | 32 | |||
| 1200 | 649 | 8000 | 62.2 | 429 | 119.1 | 821 | 26 | |
| 16000 | 63.6 | 439 | 155.6 | 1073 | 25 | |||
| All Weld Metal | Solution Heat-treated | - | 66.6 | 459 | 105.1 | 725 | 55 | |
| 1300 | 98.4 | 678 | 139.8 | 964 | 24 | |||
| 1000 | 538 | 4000 | 107.6 | 742 | 145.6 | 1004 | 26 | |
| 1000 | 60.7 | 419 | 102.5 | 707 | 24 | |||
| 4000 | 52.9 | 365 | 110.3 | 760 | 25 | |||
| 1200 | 649 | 8000 | 61.7 | 425 | 102.3 | 705 | 20 | |
| 16000 | 66.4 | 458 | 110.3 | 760 | 21 | |||



Hot Tags: hastelloy alloy s pipe, China hastelloy alloy s pipe suppliers, alloy for distillation columns, alloy for oil and gas industry, alloy for nuclear power plants, alloy for casting, alloy for chemical industry, hastelloy ss pipe