GH3128
Round steel: diameter 2mm to 1000mm
Square steel: 50mm to 600mm
Steel plate: thickness 0.5mm-12mm width 1000mm maximum
Steel pipe: outer diameter 8-800mm
Length: random length/fixed length
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of GH3128 in China. If you're going to wholesale high quality GH3128 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GNEE GH3128 High Temperature Alloy introduce
GH3128 is a Ni-Cr based solid solution strengthened deformation high temperature alloy, with a service temperature below 950℃. 16% W (W+ Mo) is added to the alloy for solid solution strengthening, and boron, cerium and zirconium are added to purify and strengthen the grain boundaries. The alloy has high plasticity, high endurance and creep strength, as well as good process performance such as oxidation resistance, stamping and welding. Its comprehensive performance is better than similar nickel-based solid solution strengthened alloys such as GH3044 and GH3536. It is suitable for making parts such as combustion chamber flame tubes and afterburner housings of aircraft engines that work for a long time at 950℃.
Available Formats:
GNEE Group offers GH3128 High Temperature Alloy in a variety of forms, including:Bars,Sheets,Tubes,Forgings.
GNEE GH3128 High Temperature Alloy Specification
GH3128 Chemical Composition:
| Element | Fe | C | Si | Mn | P | S | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| Min. | - | - | - | - | - | - | 19 | 7.5 |
| Max. | 2 | 0.05 | 0.8 | 0.5 | 0.013 | 0.013 | 22 | 9 |
GH3128 Physical Properties:
| Property | Value |
|---|---|
| Density | 8.81 g/cm³ |
| Melting Point | 1260–1400°C |
GH3128 Executive standard:
| Products | Standards |
|---|---|
| Aviation-Grade High Temperature Alloy Cold Rolled Sheet | GJB 1952-1994 |
| Welding-Grade High Temperature Alloy Cold Drawn Wire | GJB 2612-1996 |
| Aviation-Grade High Temperature Alloy Hot Rolled Plate | GJB 3317-1998 |
GNEE GH3128 High Temperature Alloy Product feature
Excellent high-temperature performance: Retains 220 MPa minimum tensile strength at 900 ℃; delivers >100 h rupture life under 39 MPa / 950 ℃, designed for long-term service up to 950–1000 ℃ and short-time exposure at 1100 ℃.
Excellent oxidation resistance: Rated fully oxidation-resistant; oxidation rate reaches 0.055 g/(m²·h) after 100 h static air exposure at 900 ℃, forming stable Cr₂O₃ oxide film with Ce addition to suppress spalling.
Excellent cold and hot workability: Hot forming window 1140–1180 ℃ with minimum finishing temperature ≥800 ℃; supports cold rolling, drawing and stamping for thin sheet and wire production, adaptable to aerospace precision forming specifications.
Excellent corrosion resistance: Resists sulfide and chloride hot gas corrosion; shows low mass loss under marine fuel gas environment, stable against oxidation and mild reducing media for aero-engine hot-section service.
GNEE GH3128 High Temperature Alloy Processing & Machining Capabilities
Hot Forming & Forging
GNEE is equipped with an 800-ton hydraulic press, hot rolling mills, and open-die forging equipment. The hot working temperature window for GH3128 is 1050–1180°C, with a final forging temperature of ≥900°C. We deliver hot-extruded bars, hot-rolled sheets/strips, and open-die forgings. All post-forging products undergo solution annealing to eliminate residual stress.
Cold Working
Cold rolling, cold drawing, and cold heading are executed on solution-treated billets, with single-pass deformation controlled at 15–25% and intermediate annealing applied between passes. Available forms include cold-rolled thin sheets (down to 0.5 mm), cold-drawn wires (down to Φ0.8 mm), and cold-heading blanks, achieving a surface roughness of Ra ≤ 1.6 μm.
Machining
CNC turning, milling, and drilling are performed using YG8/YW2 carbide or ceramic tools, with cutting speeds maintained at 30–60 m/min and flooded with emulsified coolant. We supply custom flanges, rings, and special-shaped parts machined to drawings with dimensional tolerances of IT8–IT9.
Welding
Supports GTAW (TIG), electron beam welding (EBW), and laser welding using matching GH3128 filler wire or ERNiCr-3. Welding is performed in the solution-annealed condition, followed by stabilizing annealing at 950–1000°C as required. Welds undergo 100% Liquid Penetrant Testing (PT), with Radiographic Testing (RT) applied to critical components.
GNEE GH3128 High Temperature Alloy Heat Treatment Delivery Specifications
Solution Annealing (Standard Delivery Condition)
GH3128 is a W-Mo solid-solution strengthened nickel-based superalloy, supplied in the solution-annealed condition as standard. Solution treatment is conducted at 1080–1140°C, held for 1–2 min/mm of thickness (minimum 30 minutes), followed by air cooling or water quenching. The post-solution grain size is strictly controlled within ASTM Grades 4–6.
Cooling Rate Control
Thin sheets (≤3 mm) are air-cooled, while medium-to-heavy plates, round bars, and forgings are water-quenched. The cooling rate within the critical 800→500°C temperature window is maintained at ≥100°C/s to prevent the precipitation of harmful grain-boundary phases. Transfer time from furnace to water tank is kept within ≤30 seconds.
Process Control & Quality Assurance
Heat treatment is executed in bogie-hearth resistance furnaces with temperature control precision of ±5°C. A complete heating-soaking-cooling temperature curve is recorded for every batch, accompanied by Mill Test Reports (MTR) including hardness and grain size inspection results. Optional stabilizing annealing at 950–1000°C can be provided upon contractual agreement.

GNEE GH3128 High Temperature Alloy Product application
- Aero-engine combustion chamber flame tube, additive combustion chamber shell, regulating piece
- Structural parts of gas turbine combustion chamber
- Turbine engine combustion chamber parts
- Components for booster combustion chambers
GNEE Group Factory Environment
GNEE Group GH3128 High Temperature Alloy Factory Environment


GNEE Group Packaging
GNEE Group GH3128 Alloy Packaging

GNEE Group Testing
GNEE Group High Temperature Alloy Testing

FAQ
Q: What's the terms of packing?
A: Generally,we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q: What's your delivery time?
A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit.
Q: Could you produce according to the samples?
A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.
Hot Tags: GH3128, China GH3128 suppliers, Casting High Temperature Alloy
You Might Also Like
Send Inquiry