Hastelloy Alloy W Pipe
video

Hastelloy Alloy W Pipe

Hastelloy alloy W pipe is manufactured from Hastelloy alloy W, a nickel-based superalloy that is highly resistant to corrosion and oxidation. This alloy is specifically designed for use in extremely harsh environments, including those with high concentrations of chloride ions, sulfuric acid, and other aggressive chemicals at elevated temperatures. Uses of Hastelloy Alloy W Pipe: Chemical Processing: It is widely used in the chemical processing industry, especially where there is exposure to sulfuric acid and other aggressive chemicals. Petroleum Refining: In the petroleum industry, it is used in equipment that comes into contact with hydrocarbons and acids during the refining process. Nuclear Industry: Due to its excellent resistance to high-temperature, corrosive environments, it can be used in certain applications within the nuclear industry. Marine Applications: Given its resistance to chloride and seawater, it can be used in marine applications as well.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy alloy w pipe in China. If you're going to wholesale high quality hastelloy alloy w pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

HASTELLOY W alloy (UNS N10004) is a solid-solution-strengthened super alloy that was developed primarily as a filler metal for welding of dissimilar alloys. It displays excellent dissimilar welding characteristics, and is widely used for that purpose in the gas turbine and aerospace industries. The properties of dissimilar weld joints made with alloy W are dependents upon the alloys joined, but are generally acceptable for a wide variety of combinations. Alloy W is also used as a wrought alloy for a limited number of ring-type applications in older gas turbine engines. HAYNES® 242® alloy is a more modern alloy, and should be considered as a substitute for alloy W in these ring applications (ask for publication H-3079).

Chemical Composition Requirements

The Chemical Composition of Hastelloy W, %
Ni Balance≤63.0
Cr ≤5.0
Fe ≤6.0
Co ≤2.5
Mo ≤24.0
C ≤0.12
Mn ≤1.0
Si ≤1.0

2. Mechanical Properties of Hastelloy W

Tensile Strength, min. Yield Strength, min. Elongation, min.
Mpa ksi Mpa ksi %
850 123 370 53.5 55

3. Physical Properties

Density Melting Range
g/cm3 lb/in3 °C °F
9.00 0.325 1290-1375 2350-2510

 

Hastelloy alloy w pipeHastelloy alloy w pipeHastelloy alloy w pipe

Hot Tags: hastelloy alloy w pipe, China hastelloy alloy w pipe suppliers, alloy for plating, alloy for surface treatment, alloy for industrial equipment, alloy for fuel cells, alloy for aerospace, alloy for heat exchangers

Send Inquiry

whatsapp

Phone

E-mail

Inquiry