Superalloy GH3039 Pipe
1. Good corrosion resistance
2. High temperature strength and heat resistance
3. Reliable heat fatigue resistance
4. Good processing performance
5. Excellent mechanical properties
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of superalloy gh3039 pipe in China. If you're going to wholesale high quality superalloy gh3039 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GNEE Superalloy GH3039 Pipe introduce
Superalloy GH3039 Pipe

GNEE Superalloy GH3039 Pipe
GH3039 is a high temperature alloy with excellent oxidation and corrosion resistance, as well as high strength at high temperatures. The alloy is often used in high temperature and corrosive environments. When made into tubing, GH3039 alloy tubing provides excellent performance in harsh industrial environments.
Superalloy GH3039 Pipe Size
| Outside Diameter | 3.175-219.1 mm |
| Wall Thickness | 0.5-12.7 mm |
GNEE Alloy Superalloy GH3039 Pipe Specification
Superalloy GH3039 Pipe Composition
| Element | Ni | C | Si | Mn | P | S | Al | Cr | Mo | Fe | Ti |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Content | Remainder | 0.08 Max | 0.80 Max | 0.40 Max | 0.020 Max | 0.012 Max | 0.35-0.75 | 19.0 - 22.0 | 1.80-21.30 | 3.0 Max | 0.35 - 0.75 |
Physical constants and thermal properties
| Property | Value |
|---|---|
| Density | 8.10 g/cm³ |
| Melting range | 1370–1390°C |
| Coefficient of thermal expansion (25-100°C) | 12.5 μm/m·°C (applicable at 20-800°C) |
Suggested delivery status: 1050-1080°C (WQ)
| Condition | Tensile strength (MPa) | Yield strength (MPa) | Elongation (%) |
|---|---|---|---|
| Annealing | 635 min | - | 35 min |
Gnee Steel's Available Surface Treatments
Gnee Steel can provide production process
GNEE Group Superalloy GH3039 Pipe Packaging
In order to better ensure the safety of your goods, we will provide professional, environmentally friendly, convenient and efficient packaging services.
GNEE Group Testing And Qualification Certificate
GNEE Group Superalloy GH3039 Pipe Testing And Qualification Certificate


Hot Tags: superalloy gh3039 pipe, China superalloy gh3039 pipe suppliers, machinery alloy, advanced alloy, corrosion resistant alloy, energy alloy, wear resistant alloy, Monel K500 Nickel Alloy Pipe
You Might Also Like
Send Inquiry