GH4080A High Temperature Alloy
GH4080A seamless pipe, GH4080A steel plate, GH4080A round steel, GH4080A forgings, GH4080A flange, GH4080A welded pipe, GH4080A matching welding materials, GH4080A hexagonal bar, GH4080A reducer, GH4080A elbow, GH4080A tee, GH4080A bolts and nuts, GH4080A fasteners.
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4080a high temperature alloy in China. If you're going to wholesale high quality gh4080a high temperature alloy made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GNEE GH4080 High temperature Alloy introduce
GH4080 High temperature Alloy
GH4080A is a NI-CR based precipitation hardening deformation high temperature alloy with a service temperature of less than 800℃. The alloy is mainly formed by adding aluminum and titanium elements to form a γ′ phase precipitation hardening phase. The alloy has good creep resistance and oxidation resistance in the range of 650-850℃. The alloy has good cold and hot processing properties. The main products are hot-rolled and forged bars, cold-drawn bars, hot-rolled plates, cold-rolled plates, strips and rings.
GNEE GH4080 High temperature Bright Bar Alloy Specification
Chemical composition of GH4080A
| Alloy | Element | Min (%) | Max (%) |
|---|---|---|---|
| GH4080A | Nickel (Ni) | Remainder | - |
| Chromium (Cr) | 18 | 21 | |
| Iron (Fe) | - | - | |
| Manganese (Mn) | - | 1.5 | |
| Silicon (Si) | - | 0.4 | |
| Phosphorus (P) | - | 0.02 | |
| Sulfur (S) | - | 0.015 | |
| Aluminum (Al) | 1.0 | 1.8 | |
| Titanium (Ti) | 1.8 | 2.7 | |
| Carbon (C) | 0.04 | 0.1 | |
| Cobalt (Co) | - | 2.0 | |
| Boron (B) | - | 0.008 | |
| Copper (Cu) | - | 0.2 |
GNEE GH4080 High temperature Alloy Schedule
GH4080A Series Product Information
| Product Type | Products | Dimensions | Processes | Delivery Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm (T) * W * L | Forging, hot rolling, and cold rolling | Annealed, Solution and Aging, Q+T, ACID WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm * L | Forging, hot rolling, cold rolling, Cast | Black, Rough Turning, Shot Blasting |
| Coil / Strip | Steel Coil / Steel Strip | 0.03-16.0 x 1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD: 6-219mm x WT: 0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID WASHED |



GNEE Group Factory Environment
GNEE Group GH4080 Alloy Factory Environment

GNEE Group Packaging
GNEE Group GH4080 High temperature Alloy Packaging

GNEE Group Testing
GNEE Group GH4080 Alloy Testing

FAQ
Q: What's the terms of packing?
A: Generally,we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q: What's your delivery time?
A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit.
Q: Could you produce according to the samples?
A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.
Hot Tags: GH4080A High Temperature Alloy, China GH4080A High Temperature Alloy suppliers, Casting High Temperature Alloy
You Might Also Like
Send Inquiry