Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel based alloy 20 steel pipes&tubes in China. If you're going to wholesale high quality nickel based alloy 20 steel pipes&tubes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Pipes available in the market are made up of various materials such as alloys and metals. One such pipe is the Alloy 20 Pipe that is made up of an austenitic steel material Alloy 20 Pipe manufacturers stabilize these pipes by adding niobium to the alloy. This helps in resisting intergranular corrosion. It offers good resistance to phosphoric acid, sulfuric acid, nitric acid, and aqueous salt solution.

Alloy 20 Pipes are the best solution for applications wherein chloride stress corrosion cracking is an issue. However one needs to be cautious with Alloy 20 Seamless Pipe in chloride ion containing environment as it increases the corrosion rate rapidly.
| Product Name | ASTM B729 UNS N08020 Alloy 20 Seamless Pipe |
|---|---|
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| Straight lengths | Maximum 65 ft (20 m) |
| Forms | Straight or 'U'bent Tubes |
| Surface Finish | 16 micro inch Ra (ID 0.4 micron Ra) (as drawn), 4 micro inch Ra (ID 0.1 micron Ra) (electropolished) |

Alloy 20 Welded Pipe can be formed either by hot or cold working. Hot forging material needs to be heated within the temperature range of 2100 degrees F to 2250 degrees F. Post which the Alloy 20 Pipe needs to be quenched with water. A negative effect on the stabilization of the Incoloy Alloy 20 Pipe can be obtained by heating it at a temperature below 2100 degrees F. It is also important to relieve the stress of the said pipe so that it can perform easily.