incoloy 925 Nickel Based Alloy Coil
video

incoloy 925 Nickel Based Alloy Coil

Incoloy UNS N09925 Plate, 925 Alloy Sheet, ASME SB 168 Incoloy 925 Plate, Incoloy 925 Alloy Coil, Incoloy 925 Sheet, JIS NCF Incoloy 925 Sheet. Incoloy 925 Alloy Coil Supplier, Incoloy 925 Cold Rolled Sheet, Incoloy 925 Sheet, Incoloy 925 Sheet, 925 Alloy Sheet Exporter, ASTM B 168 Incoloy 925 Gasket Dealer in China.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 925 nickel based alloy coil in China. If you're going to wholesale high quality incoloy 925 nickel based alloy coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel 925 Nickel Alloy Coil introduce

Inconel 925 Alloy Coil

Inconel 925 Nickel Based Alloy CoilInconel 925 Nickel Based Alloy Coil

The Incoloy925 is used in a variety of applications requiring a combination of high strength and corrosion resistance. Due to its resistance to sulfide stress cracking and stress corrosion cracking in hydrogen sulfide containing crude oil and natural gas, the alloy is used in downhole and surface gas well components, including tubular products, valves, suspensions, set joints, tool joints and packers. This alloy is also suitable for fasteners, Marine shafts, pump shafts and high strength piping systems.

Inconel 925 Coil is a nickel-based superalloy known for its excellent corrosion and oxidation resistance, high strength, good fabricability, and weldability. It contains chromium, iron, molybdenum and niobium as primary alloying elements. All these components impart extraordinary characteristics to the material, like creep-rupture strength at elevated temperatures and strong resistance to stress corrosion cracking in halide environments.
Inconel 925 coil is a highly versatile and corrosion-resistant alloy. It has superior strength, toughness, formability and weldability capabilities. Its superior resistance to chloride and acid-based stress cracking makes it an ideal choice for industrial applications such as chemical processing, power generation, marine components and aircraft structures. The alloy's high thermal stability makes it suitable for use in extreme temperatures, including cryogenic environments.

Specification of Incoloy 925 Sheet / Plate / Coil
Specifications : ASTM / ASME SB 168
Size : 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness : 0.1mm to 12 mm Thk
Form : Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Chemical Composition of Inconel 925 Coils

Grade C Mo Si S Cu Fe Ni Cr Al Ti
Incoloy 925 0.01 max 3 max 0.5 max 0.03 max 1.8 28 44 21 0.3 2.1

Mechanical Properties of Inconel 925 Coils

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.05 g/cm³ 1343 °C (2450 °F) Psi – 175000 , MPa – 1210 Psi – 117000 , MPa – 810 24 %

GNEE Group Factory Environment

Inconel 925 Coil

Inconel 925 Nickel Based Alloy Coil

Gnee Steel Qualification Certificate

925 Nickel Based Alloy Coil

Inconel 925 Nickel Based Alloy Coil

FAQ

1. How can we guarantee quality?

We can provide pre-production sample before mass production and final Inspection before shipment.

2. Could you provide OEM/ODM service?

Yes. Please feel free to contact us for more details.

3: Which countries do you export to?

Our products are mainly exported to Australia, Canada, Britain, the United States, Germany, Thailand, South Korea and so on.

Hot Tags: incoloy 925 Nickel Based Alloy Coil, China incoloy 925 Nickel Based Alloy Coil suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Ni36CrTiAl Plate, Uns N06600 Alloy tubing, 2 4668 Nickel Alloy Steel Coil, Alloy Steel 600 plate, Hastelloy C 22 Alloy Steel Flange

Send Inquiry

whatsapp

Phone

E-mail

Inquiry