GH4033 Alloy Round Bar
video

GH4033 Alloy Round Bar

GH4033 is a nickel–chromium precipitation hardening alloy. It is composed of 22% Chromium, 4% iron, balance nickel, 2.8% Titanium, and other elements. GH4033 alloy exhibits up to 750ºC high-temperature strength and below 900ºC oxidation resistance.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4033 alloy round bar in China. If you're going to wholesale high quality gh4033 alloy round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GH4033 Alloy Round Bar

Product Introduction

GH4033 is a high-temperature alloy with nickel-chromium as the matrix, and aluminum and titanium added to form a γ' phase dispersion-strengthened alloy. It has satisfactory high-temperature strength at 700~750℃ and excellent oxidation resistance below 900℃. The alloy has excellent cold and hot processing performance, and is mainly provided as hot-rolled bars and billets, which are used in engine rotor parts.

Chemical composition of GH4033 bar:
Grade C Mn Si S Ce Fe Ni Cr P Ti Al B
GH4033 0.03-0.08 max 0.35 max 0.65 max 0.07max 0.01 max 4.00 Remainder 19.00 – 22.00 0.015 2.4-2.8 0.60-1.0 0.01
Mechanical properties of GH4033 GB/T 14992 (2005):
Grade Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
GH4033 753 (≥) 726 (≥) 43 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 431