ASTM A276 316 Stainless Steel Hexagon Bar Hairline Finish SS Hexagonal Rod
video

ASTM A276 316 Stainless Steel Hexagon Bar Hairline Finish SS Hexagonal Rod

4m 316 stainless steel hexagon bar, ASTM A276 316 stainless steel hexagon bar, hairline finish ss hexagonal rod
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a276 316 stainless steel hexagon bar hairline finish ss hexagonal rod in China. If you're going to wholesale high quality astm a276 316 stainless steel hexagon bar hairline finish ss hexagonal rod made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Product Description:

Product Name stainless steel hexagon bar
Standard JIS, AISI, ASTM, GB, DIN
Size Diameter : S6-S65mm or as request
Length Normal long 4M, Or as your request
Surface Bright ,hairline finsh
Technics cold drawn and polishing
Application construction field, ships building industry, petroleum & chemical industries, war and electricity industries, food processing and medical industry, boiler heat exchanger, machinery and hardware fields ,etc.
Packing Export standard or as customers' requirement
Delivery time Within 15 working days, according to customers' quantities
Payment L/C or T/T
MQQ 1 Ton
Quality High Quality.SGS inspection is accepted if needed
Productivity 500 Tons/Month
Attention We will supply you good quality and bottom price and first-class service in china and hope to be your golden supplier

 

Chemical Composition:

 

Grade C Si Mn P S Ni Cr Mo
201 ≤0 .15 ≤0 .75 5. 5-7. 5 ≤0.06 ≤ 0.03 3.5 -5.5 16 .0 -18.0 -
202 ≤0 .15 ≤l.0 7.5-10.0 ≤0.06 ≤ 0.03 4.0-6.0 17.0-19.0 -
301 ≤0 .15 ≤l.0 ≤2.0 ≤0.045 ≤ 0.03 6.0-8.0 16.0-18.0 -
302 ≤0 .15 ≤1.0 ≤2.0 ≤0.035 ≤ 0.03 8.0-10.0 17.0-19.0 -
304 ≤0 .0.08 ≤1.0 ≤2.0 ≤0.045 ≤ 0.03 8.0-10.5 18.0-20.0 -
304L ≤0.03 ≤1.0 ≤2.0 ≤0.035 ≤ 0.03 9.0-13.0 18.0-20.0 -
309S ≤0.08 ≤1.0 ≤2.0 ≤0.045 ≤ 0.03 12.0-15.0 22.0-24.0 -
310S ≤0.08 ≤1.5 ≤2.0 ≤0.035 ≤ 0.03 19.0-22.0 24.0-26.0  
316 ≤0.08 ≤1.0 ≤2.0 ≤0.045 ≤ 0.03 10.0-14.0 16.0-18.0 2.0-3.0
316L ≤0 .03 ≤1.0 ≤2.0 ≤0.045 ≤ 0.03 12.0 - 15.0 16 .0 -1 8.0 2.0 -3.0
321 ≤ 0 .08 ≤1.0 ≤2.0 ≤0.035 ≤ 0.03 9.0 - 13 .0 17.0 -1 9.0 -
630 ≤ 0 .07 ≤1.0 ≤1.0 ≤0.035 ≤ 0.03 3.0-5.0 15.5-17.5 -
631 ≤0.09 ≤1.0 ≤1.0 ≤0.030 ≤0.035 6.50-7.75 16.0-18.0 -
904L ≤ 2 .0 ≤0.045 ≤1.0 ≤0.035 - 23.0·28.0 19.0-23.0 4.0-5.0
2205 ≤0.03 ≤1.0 ≤2.0 ≤0.030 ≤0.02 4.5-6.5 22.0-23.0 3.0-3.5
2507 ≤0.03 ≤0.8 ≤1.2 ≤0.035 ≤0.02 6.0-8.0 24.0-26.0 3.0-5.0
2520 ≤0.08 ≤1.5 ≤2.0 ≤0.045 ≤ 0.03 0.19 -0. 22 0. 24 -0 . 26 -
410 ≤0.15 ≤1.0 ≤1.0 ≤0.035 ≤ 0.03 - 11.5-13.5 -
430 ≤0.1 2 ≤0.75 ≤1.0 ≤ 0.040 ≤ 0.03 ≤0.60 16.0 -18.0 -

 

Application of stainless steel Hexagon Bar :

 

Petrochemical Industry Screw drill, Drilling steel, Marine drilling platform, Production platform, Oil storage ship, Floating Production Storage and Offload, lift platform, Pumps, Valves, Tubes, Pipes, etc.
Power Industry Hydropower plant, Thermal power plant, nuclear power plant, Pump, Valve, Boilers, Steam turbines, Generator sets, Pumps, Valves, Tubes, Pipes, etc.
Machinery Manufacturing Automobile manufacturing, shipbuilding, Aerospace manufacturing, Fasteners, Bolts, Nuts, Automobile parts, Medical apparatus and instruments, Pumps, Valves, Tubes, Pipes, etc.
Automobile manufacturing Axles, Instruments, Electronic parts and components, , Sensors, Turbocharger system, exhaust system, Fasteners, Bolts, Nuts, Pumps, Valves, Tubes, Pipes, etc.
Others Military industry, Environment protection, Coal and mining, etc

 

 

 

Size of our hexagon stainless steel bar in stock:

 

201 304 316L stainless steel hexagon bar
Size S6 S8 S10 S11 S12 S13 S14 S15 16 S17 S18 S19 S20 S21 S22 S24 S25 S26 S28 S29 S30 S31 S32 S33 S36 S38 S40 S41 S42 S46 S50 S55 S60 S65

 

Service:

 

Cutting our bars into any length. Cutting side is smooth without burr.

 

 

FAQ:

 

Q1. What are your company's main products ?

A1: Our main products are stainless steel plate/sheet, coil, round/square pipe, bar, channel, etc.

 

Q2. How do you control quality ?

A2: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.

 

Q3: What is the terms of packing?

A3: generally, we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers requirement.

 

Q4:What is your delivery time?

A4: For stocks, we could transport the goods to loading port within 7 days after we received your deposit

For production period, it usually takes about 15 days-30 days after receiving the deposit.

Products Show

ASTM A276 316 Stainless Steel Hexagon Bar Hairline Finish SS Hexagonal Rod 0ASTM A276 316 Stainless Steel Hexagon Bar Hairline Finish SS Hexagonal Rod 1ASTM A276 316 Stainless Steel Hexagon Bar Hairline Finish SS Hexagonal Rod 2

Hot Tags: astm a276 316 stainless steel hexagon bar hairline finish ss hexagonal rod, China astm a276 316 stainless steel hexagon bar hairline finish ss hexagonal rod suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry