1.4541 321 SS Cold-drawn Round Bar
video

1.4541 321 SS Cold-drawn Round Bar

1.4541 ss rod is a general purpose austenitic stainless steel bar with a face centered cubic structure. It is essentially non-magnetic in the annealed condition and can only be hardened by cold working. Titanium is added to supress grain boundary Chromium Carbide precipitation and reduce susceptibilty to intergranular corrosion.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4541 321 ss cold-drawn round bar in China. If you're going to wholesale high quality 1.4541 321 ss cold-drawn round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

The 1.4541 stainless round steel bar is a versatile material that finds its application in a wide range of industries. It is commonly used in the manufacturing industry, construction industry, and even in the automotive industry. This type of bar is ideal for use in buildings, bridges, and other structures due to its high strength and corrosion resistance.This is valuable in the manufacturing industry to create pipes, boilers, tanks, and other machinery components. It is also used in the automotive industry to create car bodies and auto parts by welding them with aluminum or other metals.

 

ss bar

Smooth-Rod

 

Technical data of 1.4541 ss rod bar :

Length: 100 cm - May be cut to any length.

Diameter: 14 mm

Weight: 1.23 kg

Steel grade: 1.4541 / 321

Norm: EN10088-3:2014

 

Suface Option of stainless DIN 1.4541 bar

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Common uses of Stainless Steel Round Bar 321 include:

  • Aircraft Exhaust Manifolds
  • Expansion Joints
  • Furnace Parts
  • Heat Exchangers

 

Chemical Composition of Stainless Steel 321 Rods

Grade C Mn Si P S Cr Ni Ti N
321 0.08 max. 2.00 max. 0.75 max. 0.045 max. 0.03 max. 17.0 – 19.0 9.0-12.0 5 x (C+N) min. 0.1

 

Mechanical Properties of SS 321 Bars

 

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1457 °C (2650 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

 

Customer Visit

 

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

gnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services. 

Hot Tags: 1.4541 321 ss cold-drawn round bar, China 1.4541 321 ss cold-drawn round bar suppliers, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry