316l Polished Full Round Bar Urea Grade 1.4435 ø275mm 5.5mm-500mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316l polished full round bar urea grade 1.4435 ø275mm 5.5mm-500mm in China. If you're going to wholesale high quality 316l polished full round bar urea grade 1.4435 ø275mm 5.5mm-500mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
316l Polished Full Round Bar Urea Grade 1.4435 ø275mm 5.5mm-500mm
Description
| Certification: | ISO,BV,SGS | Type: | Round |
|---|---|---|---|
| Application: | Construction | Standard: | DIN,ASTM,AISI,JIS,EN |
| Grade: | 300 Series | Shape: | Round |
| Dimensions: | 5.5mm-500mm | Surface: | Bright,Polished,black |
| Technique: | Cold Drawn&hot Rolled | Length: | Customers' Requirements |
| Packing: | Standard Seaworthy Package | ||
| High Light: |
316L Full Round Bar,Polished Stainless Steel Bar,500mm Stainless Steel Bar |
||
Full Round Bar 316L UREA Grade 1.4435 Ø275mm According The SAIPEM SPC_ON-SECTION-EXE-ENG_MAT-524-E Rev.1
1.4435
X2CrNiMo18-14-3
316L Mod
S31603
The UREA 316L grade has been specially developed for urea plant applications. It is a 316L modified stainless steel with extra – low silicon content and substantial higher molybdenum contents. The low carbon content, combined with a well balanced chemistry (low silicon and nickel content close to 14%) makes the alloy fully austenitic, free of intermetallic phase precipitations. The ferrite level is kept under 0.5% in the solution annealing and water quenched conditions. The UREA 316L grade is designed for the fabrication of lining interiors in urea units for improved corrosion resistance properties in urea – carbonate environments or complementary products (pipes, fittings…). The alloy is not designed for nitric acid application.
Mechanical Properties
| Tensile strength: | 500-700 | N/mm² |
| Yield strength 0,2% : | 200 | ≥ N/mm² |
| Elongation: | 40/30 | ≥ % |
| Hardness HB30: | 215 | ≤ HB |
Chemical Composition
| 1.4435 (316LMo) Chemical Composition | ||||||||
| Grade | C | Mn | P | S | Si | Cr | Ni | Mo |
| 1.4435 (316LMo) | %0.03 max | %2.0 max | %0.045 max | %0.015 max | %1.0 max | %17 - 19 | %12.5 - 15 | %2.5 - 3.5 |
Heat Treatment
at 1120 – 1180°C (2048 – 2156°F) followed by water quenching.
Corrosion Testing
Nondestructive testing
Welding
Typical maximum corrosion results required following different specifications after Huey tests (ASTM A262 C – five periods of 48 h.) are:
maximum weight loss lower than 3,3 μm/48 h (130 mg/dm² per 24 h.)
maximum depth for microcracks of 200 μm in the long direction and 70 μm in the transverse direction.
Marking
All material will be marked as follow:
Manufacturer's name
Material grade
Size
Heat Number
Certification
Material will be delivered with certificate EN 10204 3.1



Hot Tags: 316l polished full round bar urea grade 1.4435 ø275mm 5.5mm-500mm, China 316l polished full round bar urea grade 1.4435 ø275mm 5.5mm-500mm suppliers, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 310S Round Bar