6m 303 Stainless Steel Hex Bar Stock Bright Surface For Construction
video

6m 303 Stainless Steel Hex Bar Stock Bright Surface For Construction

Alloy 303 is a non-magnetic, austenitic stainless steel that is not hardenable by heat treatment. It is the free machining modification of the basic 18% chromium / 8% nickel stainless steel. Alloy 303 was specially designed to exhibit improved machinability while maintaining good mechanical and corrosion resistant properties Due to the presence of sulfur in the steel composition, Alloy 303 is the most readily machineable austenitic stainless steel; however, the sulfur addition does lower Alloy 303’s corrosion resistance to below that of Alloy 304. Like other austenitic grades, Alloy 303 demonstrates excellent toughness, although the sulfur does reduce this a little as well.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 6m 303 stainless steel hex bar stock bright surface for construction in China. If you're going to wholesale high quality 6m 303 stainless steel hex bar stock bright surface for construction made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Product Description:

Product Name stainless steel hexagon bar
Standard JIS, AISI, ASTM, GB, DIN
Size Diameter : S6-S65mm or as request
Length Normal long 4M, Or as your request
Surface Bright ,hairline finsh
Technics cold drawn and polishing
Application construction field, ships building industry, petroleum & chemical industries, war and electricity industries, food processing and medical industry, boiler heat exchanger, machinery and hardware fields ,etc.
Packing Export standard or as customers' requirement
Delivery time Within 15 working days, according to customers' quantities
Payment L/C or T/T
MQQ 1 Ton
Quality High Quality.SGS inspection is accepted if needed
Productivity 500 Tons/Month
Attention We will supply you good quality and bottom price and first-class service in china and hope to be your golden supplier

 

GENERAL PROPERTIES

Alloy 303 is a non-magnetic, austenitic stainless steel that is not hardenable by heat treatment. It is the free machining modification of the basic 18% chromium / 8% nickel stainless steel. Alloy 303 was specially designed to exhibit improved machinability while maintaining good mechanical and corrosion resistant properties Due to the presence of sulfur in the steel composition, Alloy 303 is the most readily machineable austenitic stainless steel; however, the sulfur addition does lower Alloy 303's corrosion resistance to below that of Alloy 304. Like other austenitic grades, Alloy 303 demonstrates excellent toughness, although the sulfur does reduce this a little as well.

APPLICATIONS

Alloy 303 is frequently used in applications that require parts to be heavily machined. Some examples include:

Nuts and bolts

Aircraft fittings

Gears

Screws

Shafts

Electrical switchgear components

Bushings

STANDARDS – ALLOY 303

ASTM/ASME ……………. UNS S30300

EURONORM ……………. FeMi35Cr20Cu4Mo2

DIN ………………………… 2.4660

CORROSION RESISTANCE

Good resistance to mildly corrosive atmospheres, but significantly less than Alloy 304

When additional sulfur is added to improve machinability, it can often slightly reduce corrosion resistance

In most dry and mild corrosive environments, Alloy 303 is comparable to other unmodified alloys

Should not be exposed to moist, marine environments as it is subject to rapid-pitting corrosion and a rust film will tend to form

Like other common austenitic stainless steels, it is subject to corrosion cracking in chloride environments above 60oC

HEAT RESISTANCE

Good oxidation resistance at temperatures up to 1700oF (927 oC)

Continuous use at temperatures above 1400oF (760oC) is not usually recommended due to carbide precipitation which can lead to irregular scaling

Does not have a low carbon content so it is also vulnerable to sensitisation

 

Chemical Properties:

 

% Cr Ni C Si Mn P S Mo Fe
303 min: 17.0
max:19.0
min: 8.0
max: 10.0
0.15
max
1.00
max
2.0
max
0.20
max
0.15 min 0.75 balance

 

Mechanical Properties:

 

Grade Tensile Strength
ksi (min.)
Yield Strength 0.2%
Offset ksi (min.)
Elongation -
% in
50 mm (min.)
Hardness
(Brinell) MAX
Hardness
(Rockwell B) MAX
303 75 30 35 228  

Products Show

6m 303 Stainless Steel Hex Bar Stock Bright Surface For Construction 2

Hot Tags: 6m 303 stainless steel hex bar stock bright surface for construction, China 6m 303 stainless steel hex bar stock bright surface for construction suppliers, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry