Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc in China. If you're going to wholesale high quality astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A36 Hot Rolled Mild Steel Checkered Plate ASTM A36 / A36M A283 GRC
Description
| Width: | 600-2500mm | Grade: | Q235B A36 |
|---|---|---|---|
| Application: | Welding Carbon Steel Materials | Technique: | Hot Rolled |
| Type: | Steel Plate | Standard: | ASTM |
| Length: | 1000-12000mm | Surface Treatment: | Black |
| Thickness: | 0.5-100mm | Material: | Q235 |
| Product Name: | Plate | Shape: | Flat Steel Plate |
| Coil Weight: | 3-8 Tons | Spangle: | Reuglar Spangle |
| High Light: |
low carbon steel plate,carbon steel sheet |
||
A36 Sheets & Plates Specifications
Specifications for A36 Sheets & Plates. If any specification is not mentioned here, please use the contact button for quick quote.
| Specifications | ASTM A36 / ASME SA36 |
| Standard | AISI, ASTM, BS, DIN, GB, JIS |
| Thickness | 0.5-100mm |
| Specialize | Shim Sheet, Perforated Sheet, B. Q. Profile. |
| Length | 2000-12000 mm |
| Form | Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
| Grade | MS A36, (UNS K02600) |
A36 Sheets & Plates Chemical Composition
| Grade | min | max |
|---|---|---|
| C | 0.25 | 0.290 |
| Cu | – | 0.20 |
| Fe | – | 98.0 |
| Mn | – | 1.03 |
| P | – | 0.040 |
| Si | – | 0.280 |
| S | – | 0.050 |
Mechanical Properties of A36 Sheets & Plates
| Properties | Metric | Imperial |
| Density | 7.85 g/cm3 | 0.284 lb/in3 |
| Tensile Strength, Ultimate | 400 – 550 MPa | 58000 – 79800 psi |
| Tensile Strength, Yield | 250 MPa | 36300 psi |
| Elongation at Break (in 200 mm) | 20.0 % | 20.0 % |
| Elongation at Break (in 50 mm) | 23.0 % | 23.0 % |
| Modulus of Elasticity | 200 GPa | 29000 ksi |
| Bulk Modulus (typical for steel) | 140 GPa | 20300 ksi |
| Poissons Ratio | 0.260 | 0.260 |
| Shear Modulus | 79.3 GPa | 11500 ksi |
A36 Sheets & Plates – Equivalent Grades
| STANDARD | MS A36 |
|---|---|
| WERKSTOFF NR. | 50049 3.1 |
| UNS | K02600 |
A36 Coils
A36 UNS K02600 Coils
A36 WERKSTOFF NR. 50049 3.1 Coils
A36 Strips
A36 UNS K02600 Strips
A36 WERKSTOFF NR. 50049 3.1 Strips
A36 Foils
A36 UNS K02600 Foils
A36 WERKSTOFF NR. 50049 3.1 Foils
A36 Shim Sheet
A36 UNS K02600 Shim Sheet
A36 WERKSTOFF NR. 50049 3.1 Shim Sheet



Hot Tags: astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc, China astm a36 hot rolled mild steel checkered plate astm a36 / a36m a283 grc suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate
You Might Also Like
Send Inquiry