CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width
video

CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society . 2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ccs ah36 dh36 steel plate for ships with thickness 6mm 8mm 2000mm width in China. If you're going to wholesale high quality ccs ah36 dh36 steel plate for ships with thickness 6mm 8mm 2000mm width made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width

Description

Grade: AH36 DH36 EH36 Width: 1000-2500mm
Length: 2000-12000mm Class: CCS BV GL AB KS
Thickness: 3-200mm Type: Plate
High Light:

CCS Steel Plate For Ships

,

8mm Ship Steel Plate

,

AH36 DH36 Ship Steel Plate

Shipbuilding And Offshore Engineering Steel Ah32 Ah36 Ah40 Provide Cutting And Relevant Service

 

Commodity Marine Grade Steel AH32 AH36 Ship Building Steel Plate
Standard CCS,ABS,GL,BV,DNV,NK,LR,KR,RINA
Grade

A/B/D/E, A32/D32/E32/F32, A36/D36/E36/F36, A40/D40/E40/F40,

NVA420/D420/E420, NVA460/D460/E460, NVA500/D500/E500, NVA550/D550/E550….

Thickness 2-300mm
Width 1000-3000mm
Length 1000-12000mm or as your request
Surface Clean, finishing,blasting and painting according to customer requirement
Delivery States Hot-rolled, Controlled rolling, Normalizing, Annealing, Tempering,
Quenching, N+T, Q+T,and other delivery states are available as required
Certificate API,ISO,SGS,BV,CE etc
Quality MTC will be provided with goods, third part inspection is acceptable
Package Standard export seaworthy package,suit for all kinds of transport; or as required.
Container 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High)
Application Widely used in a variety of architectural and engineering structures,such as
1.) metal constructions such as buildings,bridges,ships;
2.) transmission tower, reaction tower;
3.) lifting transportation machinery;
4.) industrial furnace;boilers
5.) container frame, warehouse goods shelves, etc

 

CCSA CCSB AH36 shipping building steel plate

 

Specification

Ah36 steel plate is used for shipbuiling&platform.The shipbuilding steel plate grade AH36 is the high tensile strength steel. Ah32 shipbuilding steel has good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and welding properties. ASTM A131 Ah36 steel plate can be used in the manufacture of the ship's hull structure whose weight is more than 10000 tons.

AH36 Shipbuilding steel plate specification:
Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm.

Chemical Composition % of Ah36 shipbuilding steel plate

 


Grade
C
max
Si
max
Mn P
max
S
max
Als
min
Ti
max
Cu
max
Cr
max
Ni
max
Mo
max
AH36 0.18 0.50 0.90-1.60 0.035 0.035 0.015 0.02 0.35 0.20 0.40 0.08

 

Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.36% (thickness ≤ 50mm),≤0.38%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.

 

Mechanical Property of Ah36 shipbuilding steel plate

 


Grade
Rm
(MPa)
Re(MPa) min A% min Akv/J min
AH36 440-570 315 22 E.T °C Thickness (mm)
0 ≤ 50 >50-70 >70-100
L C L C L C
31 22 38 26 46 31

 

Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.

 

Ah36 steel plate Condition Of Delivery

 


Grade
Fine grains elements category The thickness of steel
≤ 12 >12.5-20 >20-25 >25-35 >35-50 >50-100
AH36 Nb+V or V Plate/
sheet
A(50) N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel N(50),CR(50),TM(50),AR*(25) -
Al or Al+Ti Plate/
sheet
A(50) AR*(25) -
N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel A(50) N(50),CR(50),TM(50),AR*(25) -

 

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

 

CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width 0CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width 1CCS AH36 DH36 Steel Plate For Ships With Thickness 6mm 8mm 2000mm Width 2

Hot Tags: ccs ah36 dh36 steel plate for ships with thickness 6mm 8mm 2000mm width, China ccs ah36 dh36 steel plate for ships with thickness 6mm 8mm 2000mm width suppliers, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate