304H Stainless Steel Plate
video

304H Stainless Steel Plate

304H is the stainless Steel alloy known for an economical option with the versatile property of corrosion resistance. It is more suitably employed in general purpose applications with a wide range. It is enhanced SS 304 grade with a higher carbon value. Thus increase in strength is acquired at high temperatures. It gets more vulnerable to welding carbide precipitation.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 304h stainless steel plate in China. If you're going to wholesale high quality 304h stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

304H is the stainless Steel alloy known for an economical option with the versatile property of corrosion resistance. It is more suitably employed in general purpose applications with a wide range. It is enhanced SS 304 grade with a higher carbon value. Thus increase in strength is acquired at high temperatures. It gets more vulnerable to welding carbide precipitation.

Superior carbon made these SS 304H plates more resistant to heat. These are recommended for higher tensile at stress conditions. Our SS 304H sheets are better yield strength consuming with excellent mechanical and thermal properties in carbide precipitation avoiding range.

Grade C Mn Si P S Cr Mo Ni N
SS 304H 0.10 max 2.0 max 0.75 max 0.045 max 0.03 max 18 – 20 - 8 – 10.5 -

 

4 298

Mechanical Properties
Density: 8.0 g/cm³
Melting Point: 1400 °C (2550 °F)
Tensile Strength: Psi – 75000 , MPa – 515
Yield Strength (0.2% Offset): Psi – 30000 , MPa – 205
Elongation: 40 %

4 228

They are accurately dimensioned and available in various forms like perforated, Plain, Shim Sheet, Chequered Plate, Strip, etc. These plates hold larger short term, as well as long term, creep strength. Grade 304H provides higher strength to sheets at eminent temperatures. Therefore it is suggested in structural applications at temperatures nearly 500°C to 800°C. They are utilized in various pressure applications with excellent hardness.

NEXTGEN STEEL & ALLOYS supplies the broad extent of plates and sheets for national and global application industries. These 304H Plates are available in various categories. Our sheets are used in various working areas like heater segments, honeycombs parts, gas turbine segments, pressure vessels, tanks, heat exchangers, piping, fittings and flanges. They are additionally utilized in inorganic and natural arrangements. Our plates offer extraordinary opposition highlight that makes them useful for all environmental elements and applications.

Hot Tags: 304h stainless steel plate, China 304h stainless steel plate suppliers, Corrugated SS Roof Sheet, 400 2 4360 Alloy Pipe, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry