High Tensile Strength E350C Steel Plate S335J2+N Hot Rolled Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of high tensile strength e350c steel plate s335j2+n hot rolled plate in China. If you're going to wholesale high quality high tensile strength e350c steel plate s335j2+n hot rolled plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
High Tensile Strength E350C Steel Plate S335J2+N Hot Rolled Plate
Description
| Width: | 600-2500mm | Grade: | S335J2+N |
|---|---|---|---|
| Technique: | Hot Rolled | Type: | Steel Plate |
| Standard: | ASTM,GB,AISI,JIS,DIN | Length: | 1000-12000mm |
| Surface Treatment: | Hot Finished | Special Use: | High-strength Steel Plate |
| Thickness: | 0.5-100mm | Zinc Coating: | Mild Steel Plate Can Be Proce |
| High Light: |
stainless steel coil stock,cold rolled stainless steel coil |
||
Standard Specification
Standard
EN 10025-2:2004
Width
1000mm-4500mm
Thickness
3mm-150mm
Impact tested :
-52° C
Length
3000mm -18000mm
Process
Hot-Rolled (HR)
Destructive and Non-Destructive Testing
Mechanical examining like tensile, Elongation
and reduction of area.
Chemical examination-Spectro analysis
Impact analysis
Hydrostatic analysis
Positive material recognition
X-ray test
Firmness test
S355J2+N / E350 C Plate Processing
Cutting
Forming Drilling/ Machining
Grinding
Testing
S355J2+N Equivalent Grades :
| Grade | DIN | ASTM | EN | JIS | Material no. |
| S355 J2+N | 17100 St52-3N |
A572-50 | 10025-2:2004 | G3106 SM490YB |
1.0577+N |
Chemical Composition of S355J2+N / E350 C Plate
| Grade | C | Si | Mn | S | P | C.E |
| S355 J2+N | 0.22 max | 0.55 max | 1.60 max | 0.035 max | 0.035 max< | 0.047 max |
| (E350) Fe 490 | 0.20 max | 0.45 max | 1.50 max | 0.045 max | 0.045 max< | - |
Mechanical Properties of S355J2+N / E350 C Steel Plate
| Grade | Thickness (mm) | Yield Strength Rehmin (N / mm²) | Tensile Strength Rmmin (N / mm²) | Elongation A5 min(%) | Impact Values Charpy-V-Notch LongitudinalAverage from 3 Speimens Thk.>10<150mm. |
| S355J2+N | 3<thk<100 | 315-355 | 490-630 | max 22 | 27 Joules at -20 C |
| E350 | <20mm->40mm | 320-350 | 490 | 22% | 25 Joules at -20 C |


Hot Tags: high tensile strength e350c steel plate s335j2+n hot rolled plate, China high tensile strength e350c steel plate s335j2+n hot rolled plate suppliers, SS410 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate, 400 2 4360 Alloy Pipe