Hastelloy C2000 and C276 are both nickel-chromium-molybdenum alloys known for their corrosion resistance, but they have different chemical compositions and performance characteristics. Hastelloy C2000 is designed to resist a wider range of corrosive media, including both reducing and oxidizing environments, and has better resistance to pitting and crevice corrosion than C276. C276 is known for its resistance to localized corrosion, especially in chloride-containing environments.

Gnee Steel
What is Hastelloy C2000?
HASTELLOY C-2000 alloy
It is a highly corrosion-resistant nickel-chromium-molybdenum alloy. One of the characteristics of this material is that the copper content is low but effective without reducing its thermal microstructural stability.

Hastelloy C2000:
Composition:
It has a high chromium content (23%) and a small amount of copper (1.6%), which enhances its resistance to reducing acids such as sulfuric acid.
Corrosion Resistance:
Exhibits excellent resistance to both oxidizing and reducing environments, making it a versatile choice for a wide range of chemical processing applications.
Applications:
Used in chemical processing equipment, pollution control systems and other applications requiring resistance to a wide range of corrosive substances.
Hastelloy C276:
Composition:
It is characterized by a high molybdenum content (15-17%), a high tungsten content (3-4.5%), and is extremely resistant to reducing agents such as hydrochloric acid.
Corrosion Resistance:
Well known for its excellent resistance to pitting and crevice corrosion, especially in chloride containing environments.
Applications:
Commonly used in flue gas desulfurization systems, chemical processing equipment and other applications involving severe corrosive conditions.

Gnee Steel is a supplier of Hastelloy C2000 And C276 Alloy, covering tubes: seamless tubes: size: 4 - 219 mm; thickness: 0.5 - 20 mm; welded tubes: size: 5.0 - 1219.2 mm; thickness: 0.5 - 20 mm, plates: plate thickness 0.1 to 100 mm; plate width 10-2500 mm, strips, alloy round bar size: diameter 3-800 mm;, flat bar size: thickness 2-100 mm; width: 10-500 mm, hexagonal bar size: 2-100 mm;, wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Hastelloy C2000 And C276 Alloy, pipes, tubes, plates, strips, sheets, round bars, flat bars, forged billets, hexagons, wires and extruded profiles. You are welcome to contact us anytime to get a quote at ss@gneesteel.com