Hastelloy C-2000
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c-2000 in China. If you're going to wholesale high quality hastelloy c-2000 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy C-2000, also known as Alloy C-2000, UNS No. N06200, W. Nr. 2.4675, is a copper-containing Ni-Cr-Mo alloy that has excellent resistance to a wide range of corrosive chemicals, including sulfuric acid, hydrochloric acid and other aggressive media.
Hastelloy C-2000 Usable Range
| Bars and Rods | Seamless pipes and tubes | Welded pipe and tube | Plates, sheets and strips | Forgings | Pipe fittings |
|
ASTM B 574/ASME SB 574 |
ASTM B 622 / ASME SB 622 |
ASTM B 626 /ASME SB 626, ASTM B 619 / ASME SB 619 |
ASTM B 575/ASME SB 575 |
ASTM B 564 /ASME SB 564, B472/SB472, B462/SB462 |
ASTM B 366/ASME SB 366, B462/SB462 |
Please contact us at ss@gneesteel.com for details.
Hastelloy Alloy C-2000 Applications
Chemical Processing Equipment: Used in the manufacture of reactors, heat exchangers and piping systems for handling corrosive chemicals such as sulfuric acid, hydrochloric acid and phosphoric acid.
Pollution Control: The alloy is used in flue gas desulfurization systems, scrubbers and other pollution control equipment, where resistance to corrosive environments is critical.
Pulp and Paper Industry: The alloy is used in the manufacture of equipment that handles corrosive chemicals during pulp and paper production.
Hastelloy C-2000 Alloy specification
Chemical composition
|
(Ni) |
margin |
|
(Co) |
Up to 2% |
|
(Cr) |
22-24% |
|
(Mo) |
15-17% |
|
(Cu) |
1.3-1.9% |
|
(Fe) |
Max 3.0% |
|
(C) |
Max 0.01% |
|
(Mn) |
Max 0.50% |
|
(Al) |
Max 0.5% |
|
(S) |
Max 0.01% |
|
(Si) |
Max 0.08% |
|
(P) |
Max 0.025% |
Physical properties
| density |
8.50 g/cm3 (0.307 lb/in.3) |
| Melting point range |
1328-1358°C (2422-2476°F) |
| Coefficient of Thermal Expansion (@ 25-100°C/ 77-212°F) |
12.4 μm/m°C (6.89 μin/in°F) |
| Thermal conductivity |
9.10 W/mK (63.2 BTU in/hr.ft².°F) |
Mechanical properties
| thickness | tensile strength | Yield Strength | Elongation | |||
| At 0.2% offset | ||||||
|
mm |
in. |
MPa |
ksi |
MPa |
ksi |
in 50 mm (2 in.), % |
|
1.6 |
0.063 |
752 |
109 |
358 |
52 |
64 |
|
3.2 |
0.125 |
765 |
111 |
393 |
57 |
63 |
|
6.4 |
0.25 |
779 |
113 |
379 |
55 |
62 |
|
13 |
0.5 |
758 |
110 |
345 |
50 |
68 |
|
25 |
1 |
752 |
109 |
372 |
54 |
63 |
Alloy C-2000

Professional Supplier-GNEE

First-class Hastelloy C-2000 production process

Top-quality nickel alloy C-2000 product quality

FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.