What Is C276 Material Used For Welding?

What is C276 material used for welding?

 

ERNiCrMo-4 Nickel Alloy C276 is used for welding materials of similar chemical composition as well as dissimilar materials such as nickel-based alloys, steels and stainless steels. The alloy can also be used to clad steel with nickel-chromium-molybdenum weld metal. The higher molybdenum content provides effective resistance to stress corrosion cracking, pitting and crevice corrosion.

What is C276 material used for welding?What is C276 material used for welding?

C Mn Fe P S Si Cu Ni Co Cr Mo V W Other
0.02 1.0 4.0-7.0 0.04 0.03 0.08 0.50 Rem 2.5 14.5-16.5 15.0-17.0 0.35 3.0-4.5 0.5