The development prospects of the non-oriented electrical steel industry are very good. Because it brings many benefits to enterprises when used, it is favored by customers. In order to let everyone know more, we will talk about it next. Let's take a look at the characteristics of non-oriented electrical steel, hoping to help more people.
Today, there are still many people who do not understand some basic information about non-oriented electrical steel, so as a manufacturer, it is necessary for us to briefly explain it. In fact, non-oriented electrical steel is now mainly used for large and medium-sized motors, generators, and household appliances. Cores for electric motors and micromotors, ballasts and small transformers. The main requirements for the magnetic properties of non-oriented electrical steel are low specific total loss and high magnetic polarization. Of course, everyone must know that it is smaller than the total loss, which can save a lot of energy and extend the working life of the motor. Large magnetic polarization means strong magnetizing ability, reduced core excitation current, and reduced total loss and copper loss. Specific total losses and magnetic polarization are not only related to the chemical composition, but also mainly related to the internal organization of its operation. In order to have a deeper understanding of the characteristics of non-oriented electrical steel, better guide production, and improve product quality, a comprehensive study was conducted on cold-rolled non-oriented electrical steel in 2010.
Nowadays, non-oriented electrical steel increases the resistance and reduces the total specific loss, but silicon is not a magnetic element. Silicon reduces the saturation magnetization intensity and correspondingly reduces the magnetic polarization, which is detrimental to magnetism. At the same time, too high silicon content will make the steel brittle and make cold working difficult, so we also see that the upper limit of silicon content of cold-rolled electrical steel is usually set at about 3.0%. The role of non-oriented electrical steel is similar to that of silicon. Aluminum can reduce the γ phase area, coarsen grains, and increase resistance, thereby reducing magnetic anisotropy, specific loss and magnetic polarization. The effects of strength and hardness are less pronounced than with silicon. Both silicon and aluminum control the mechanical and magnetic properties of non-oriented electrical steels by controlling grain size or texture. Of course, it can also be seen from the average values of mechanical properties and magnetic properties. After plotting the grain size, mechanical properties and magnetic properties of different grades of non-oriented electrical steel into curves, it can be concluded that W600, W800 and W1300 crystal The particle size increases in sequence, that is, the grain size decreases in sequence. The company is committed to the expansion and development of domestic and foreign markets, using both online Internet e-commerce platforms and offline physical sales to go hand in hand.
The content of the above article is some relevant information introduced by the editor about the characteristics of non-oriented electrical steel. If you didn't know it before, you can take a look now. In the next issue, I will tell you some knowledge points related to it. Remember to come and watch. Of course, our company's products can still meet these needs. We welcome here to establish long-term cooperative relationships with friends from all over the country.
Non oriented silicon steel