Inconel 600 Round Bar

Understanding Inconel 600 Round Bar High Temperature Performance
Inconel 600 Round Bar is a nickel-chromium alloy with excellent resistance to oxidation and corrosion at high temperatures. Its excellent machinability and weldability make it an ideal choice for applications requiring high strength and durability in high temperature environments.
What temperatures can Inconel alloy 600 withstand?
The hot working temperature range for Inconel alloy 600 is 1600–2250°F (870–1230°C). High-intensity working requires temperatures between 1900–2250°F (1040–1230°C), while light working can be performed at temperatures as low as 1600°F (870°C).

Chemical composition of Inconel 600 bar
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
600 Alloy Rod Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
Applications for Inconel 600 bar and rod:
Sulfuric, phosphoric, and acetic acid processing plants.
Pulp and paper processing.
Gas scrubber components.
Seawater cooling equipment.
Refinery components.
Electrostatic precipitator wiring.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.