Nickel Alloy 625 Precision Ground Rods Learn More

 
 
 
Nickel Alloy 625 Precision Ground Rods Learn More
Inconel 625 precision ground rods
01.

Nickel Alloy 625 Precision Ground Rods Learn More

Nickel Alloy 625 Rod (Inconel 625) is a non-magnetic nickel-chromium-molybdenum alloy rod with excellent corrosion resistance. It maintains high strength at cryogenic temperatures down to 2000°F (1093°C) and maintains good oxidation resistance up to 1800°F (982°C). Inconel 625 precision ground rods are manufactured to tight dimensional tolerances for applications requiring high precision, such as those in the aerospace and chemical processing industries, which often face extreme temperatures and corrosive environments.

02.

spary read laser welding technology

Dual-station multi-axis intelligent working platform;

 

Synchronised CCD precision positioning;

 

High welding precision, high consistency of welding joints,especially suitable for high precision electronic device processes.

news-800-400

Standard size and Specification Inconel Precision 625 Round Bar

Specifications ASTM B446 / ASTM SB446
size 2-100mm A/F
Square bar size 4 to 100mm
Flat bar size Thickness: 2 -100mm
Width: 10 to 500mm
Round bar size Diameter: 3-~800mm
Rectangles Size 33 x 30mm to 295 x 1066mm
Angle bar size 3mm*20mm*20mm~12mm*100mm*100mm
Section 3.0 to 12.0mm thickness
Channel Bar 80 x 40mm to 150 x 75mm section; 5.0 to 6.0mm thickness
Hollow Bar 32mm OD x 16mm ID to 250mm OD x 200mm ID)
Billet Size 1/2" to 495mm Diameter

 

Inconel 625 Round Bar Chemical Structure

Grade C Mn Si S Cu Fe Ni Cr
Inconel 625 0.10 max 0.50 max 0.50 max 0.015max – 5.0 max 58.0 min 20.0 – 23.0

 

Mechanical Properties Chart Alloy 625 Round Bar

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 625 8.4 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

 

625 Precision Ground Rod Applications:
Aerospace: Used in the manufacture of components for jet engines and turbine shafts.
Marine: Ideal for seawater applications, such as ship fasteners and components in propulsion systems.
Chemical Industry: Suitable for reactor supports, furnace hardware, and chemical plant equipment due to its resistance to various corrosive conditions.
Other Industries: Used in nuclear facilities, oil drilling, and other high-performance applications.

 

Precision Grinding Process:
Tight Tolerances: The precision grinding process achieves tight dimensional tolerances and a smooth surface, which is critical for many specialized applications.
Enhanced Surface Finish: This process provides a bright or polished finish, enhancing the appearance and functionality of the rod.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications, and we can provide customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneemetal.com.