Dec 25, 2023 Leave a message

Monel400(N04400) Physical Performance Parameters Introduction Monel400(N04400) Application Fields

Monel400(N04400) physical performance parameters introduction Monel400(N04400) application fields

 

Monel 400 (N04400) Monel alloy is a corrosion-resistant alloy with the largest usage, the most wide range of uses, and excellent comprehensive properties. This alloy has excellent corrosion resistance in hydrofluoric acid and fluorine gas media, and also has excellent corrosion resistance against hot concentrated alkali liquid. It is also resistant to corrosion from neutral solutions, water, seawater, atmosphere, organic compounds, etc. An important feature of this alloy is that it generally does not produce stress corrosion cracking and has good cutting performance.

The chemical composition of Monel400 alloy is mainly composed of 30% Cu and 65% Ni plus a small amount of Fe (1%-2%). The organizational structure is a typical single-phase austenite structure. Since nickel and copper can dissolve each other in any proportion, there is generally no intermetallic phase precipitation.

Monel400(N04400) physical performance parameters introduction Monel400(N04400) application fields

Monel400(N04400) physical performance parameters introduction Monel400(N04400) application fields

When observing the structure of this alloy under non-etching conditions under a metallographic microscope, it can be seen that there are very dispersed non-metallic inclusions, such as sulfides and silicates, on the austenite matrix. Under certain conditions, the presence of carbides may also be observed. Due to differences in chemical composition, it can have a variety of alloy grades, but there is no significant difference in corrosion resistance between them. Monel400 alloy is more resistant to corrosion by reducing media than pure nickel, and more resistant to corrosion by oxidizing media than pure copper.

Monel 400 physical properties:

Density 8.83 g/cm3

Melting point 1300-1390 ℃

Monel 400(N04400) Mechanical properties of Monel alloy:

1. Monel 400 (N04400) Monel alloy tensile strength: σb≥450Mpa.

2. Monel 400 (N04400) Monel alloy yield strength: σb≥170Mpa.

3. Monel 400 (N04400) Monel alloy elongation: δ≥30%.

Monel 400 (N04400) Monel alloy application fields:

Marine heat exchangers, desalination equipment, salt production equipment, marine and chemical processing equipment, propeller shafts and water pumps, gasoline and water tanks, etc.

 