Monel 400 nickel-copper alloy cold-worked seamless pipe

Monel 400 nickel-copper alloy cold-worked seamless pipe
Monel 400 cold-finished seamless pipe is a high-strength, corrosion-resistant nickel-copper alloy (UNS N04400) that performs exceptionally well in marine environments, at high temperatures, and in corrosive media such as seawater, hydrochloric acid, and hydrofluoric acid. Cold working increases its mechanical strength, making it suitable for demanding applications such as chemical processing, offshore engineering, and oil and gas. It can also be used as components in heat exchangers, pumps, and springs.
What is the difference between Monel and Nickel 400?
400 alloy is primarily composed of copper (67%) and nickel (25%). It also contains trace amounts of iron, manganese, carbon, and silicon. In contrast, Monel 400 has a slightly different composition. It is composed of 63% nickel and 34% copper, with small additions of iron, manganese, and silicon.

Overview of MONEL400/UNS N04400 Cold-Worked Seamless Pipe
Monel 400 pipe is a nickel-copper alloy resistant to high-temperature seawater and steam, as well as saline and alkaline solutions. Monel 400 pipe is a nickel-copper alloy with excellent corrosion resistance in a wide range of media. It offers good corrosion resistance, excellent weldability, and medium to high strength. This alloy is widely used in a variety of applications. It exhibits excellent resistance to fast-flowing brackish or seawater, and is particularly resistant to degassed hydrochloric and hydrofluoric acids. The alloy is slightly magnetic at room temperature. Monel 400 pipe is widely used in the chemical, petroleum, and marine industries.
Properties of MONEL400/UNS N04400 Cold-Worked Seamless Pipe
It offers corrosion resistance in a wide range of marine and chemical environments, from pure water to non-oxidizing mineral acids, salts, and alkalis.
The alloy is more resistant to nickel under reducing conditions and better than copper under oxidizing conditions, but its resistance in reducing media is better than in oxidizing media. It exhibits good mechanical properties at temperatures ranging from sub-zero to approximately 480°C.
It exhibits good resistance to sulfuric and hydrofluoric acids. However, aeration can lead to accelerated corrosion rates. It can handle hydrochloric acid, but the presence of oxidizing salts greatly accelerates corrosion.
The alloy is resistant to neutral, alkaline, and acidic salts, but has poor resistance to oxidizing acidic salts (such as ferric chloride).
It exhibits excellent resistance to chloride ion stress corrosion cracking.
Chemical Composition of MONEL 400 Pipe
| Ni | C | Mn | S | Si | Cu | Fe | |
| Max | 0.3 | 2.00 | 0.024 | 0.5 | 34.0 | 2.50 | |
| Min | 63.0 | 28.0 |
Mechanical Properties of UNS N04400 Pipe
|
Condition & Size |
Tensile Strength, min. ksi [MPa] |
Yield Strength, min. ksi [MPa] |
Elongation, min. % |
|---|---|---|---|
| *A | 70 [480] | 28 [195] | 35 |
| *B | 70 [480] | 25 [170] | 35 |
| *C | 85 [585] | 55 [380] | 15 |
Production and Processing
Raw Materials: High-purity nickel, copper, iron, and manganese are melted to form a stable alloy.
Casting and Hot Working: The molten alloy is cast into billets and then hot-rolled into intermediate shapes.
Cold Working: The billets are then cold worked (drawn or rolled) to refine the grain structure and increase mechanical strength until the desired full hard state is reached.
Heat Treatment: Annealing or stress relieving can be performed to relieve stresses, restore ductility, and achieve the desired combination of strength and ductility.
Applications
Marine: Used in pumps, valves, marine equipment, propeller shafts, and seawater equipment.
Chemical Processing: Suitable for process vessels, piping, heat exchangers, and equipment handling acids such as hydrochloric and hydrofluoric acids.
Other Uses: Used in gasoline and fresh water tanks, crude oil stills, and components in the explosives industry.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.