Mechanical Properties Of GH706 Alloy

Mechanical properties of GH706 alloy

 

GH706 Overview

GH706 alloy is a precipitation hardening Fe-Ni-Cr based alloy. Because it has a reasonable chemical composition, compared with other high-temperature alloys, GH706 alloy has excellent machining performance and weldability, and has a certain strength and toughness, and has good resistance in a higher and wider medium range. Oxidation and corrosion resistance, low production cost. It is used in a variety of applications, such as where high strength is required but an easy-to-process material is required. In the aerospace industry, GH706 is used as a raw material for engine mounts and fasteners. In addition, this alloy is often used as a raw material for turbine disks in large industrial gas turbines. Therefore, its existence has great economic and technical value. , can be made into bars, forgings, rings, sheets, strips and other products for supply.

Mechanical properties of GH706 alloy

Mechanical properties of GH706 alloy

Material grade GH706.

Similar grade Inconel 706 (USA).

GH706 Formulation of heat treatment system

The composition of GH706 alloy is similar to that of GH4169 alloy, and its properties are also close. As it can be used at around 650℃

The material used is a promising alloy. Since the properties of the alloy are directly affected by the heat treatment system, it is very important to develop a reasonable heat treatment system to improve the properties of the alloy. The standard heat treatment system of GH706 alloy is: 980℃ insulation for 1 hour, air cooling + 845℃ insulation for 3 hours, air cooling + 720℃ insulation for 8 hours, furnace cooling to 620℃ insulation for 8 hours.

Variety specifications and supply status We can produce and supply bars, forgings, rings, sheets, strips and other products. Bars and forging blanks for hot working are delivered without heat treatment and lathe.