Inconel MA758 nickel-based alloy
Inconel MA758 nickel-based alloy
1. Chemical composition (wt% provided):
C Cr Ni Al Ti Fe Y2O3
0.05 30.0 Margin 0.3 0.5 1.0 0.6
2. Physical properties Shunteng Metal provides:
Density (8.14g/cm3) Melting point (1375°C)
3. Minimum mechanical properties of the alloy at room temperature:
Status Yield strength (MPa) Tensile strength (MPa) Elongation %
Rod 560 949 27
Plate 680 1030 14
4. Characteristics:
1. Good antioxidant properties;
2. Good resistance to glass liquid
5. Application areas:
Applications and heat treatment and application areas with the most stringent requirements for high-temperature metals and alloys, iron melting furnace components such as furnace rollers, clamps, tools, etc.
Other components used in heat treatment processes, fuel atomization applications in diesel engines, etc.
Inconel MA758 chemical composition:
C Cr Ni Al Ti Fe Y2O3
0.05 30.0 Margin 0.3 0.5 1.0 0.6
Inconel MA758 corresponding brand: Alloy MA758
Inconel MA758 physical properties:
Density (g/cm3) Melting point (°C)
8.14 1375
Minimum mechanical properties of Inconel MA758 alloy at room temperature:
Status Yield strength (MPa) Tensile strength (MPa) Elongation %
Rod 560 949 27
Plate 680 1030 14
Inconel MA758 features:
1. Good antioxidant properties
2. Good resistance to glass liquid
Inconel MA758 application areas: applications and heat treatment and applications with the most stringent requirements for high-temperature metals and alloys, iron melting furnace components such as furnace rollers, clamps, tools, etc.


2. Physical properties:
Density (g/cm3)
Melting point (°C)
8.14
1375
3. Minimum mechanical properties of the alloy at room temperature:
state
Yield strength (MPa)
tensile strength
(MPa)
Elongation
%
Rod
560
949
27
plate
680
1030
14
4. Characteristics:
1. Good antioxidant properties;
2. Good resistance to glass liquid
5. Application areas:
Applications related to heat treatment and application areas with the most stringent requirements for high temperature metals and alloys, etc. Iron melting furnace components such as furnace rollers, clamps, tools, etc.
Other components used in heat treatment processes, fuel atomization applications in diesel engines, etc.