1. Chemical composition (wt% provided):

C Cr Ni Al Ti Fe Y2O3
0.05 30.0 Margin 0.3 0.5 1.0 0.6

2. Physical properties Shunteng Metal provides:

Density (8.14g/cm3) Melting point (1375°C)

3. Minimum mechanical properties of the alloy at room temperature:

Status Yield strength (MPa) Tensile strength (MPa) Elongation %
Rod 560 949 27
Plate 680 1030 14

Inconel MA758 nickel-based alloy

Inconel MA758 nickel-based alloy

4. Characteristics:

1. Good antioxidant properties;
2. Good resistance to glass liquid

5. Application areas:

Applications related to heat treatment and application areas with strict requirements for high temperature metals and alloys, iron melting furnace components such as furnace rollers, clamps, tools, etc.
Other components used in heat treatment processes, fuel atomization applications in diesel engines, etc.

Inconel MA758 chemical composition:

C Cr Ni Al Ti Fe Y2O3

0.05 30.0 Margin 0.3 0.5 1.0 0.6

Inconel MA758 corresponding brand: Alloy MA758

 