Aug 29, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

High-Temperature Resistant Inconel 600 Alloy Round Bar Encyclopedia

 
 
 
High-temperature resistant Inconel 600 alloy round bar encyclopedia
High-temperature resistant Inconel 600 alloy round bar encyclopedia
01.

High-temperature resistant Inconel 600 alloy round bar encyclopedia

Inconel 600 alloy round bar is a high-temperature resistant nickel-chromium-iron alloy (UNS N06600) bar known for its exceptional strength, corrosion, and oxidation resistance, even at extreme temperatures up to 2000°F (1093°C). Its excellent mechanical properties, including high tensile and fatigue strength, make it suitable for applications such as chemical processing, nuclear power, aerospace, and food processing, where high-reliability, non-magnetic, corrosion-resistant components are critical.

02.

What is the ASTM standard for Inconel 600 Bar?

Inconel 600 round bar is composed of 72% nickel, 14% chromium, iron, carbon, manganese, sulfur, silicon, and copper. This material has a high melting point of 1413°C. The minimum yield strength of ASTM B166 UNS N06600 round bar is 310 MPa, and the minimum tensile strength is 655 MPa.

Inconel 600

Inconel 600 Round Bar Standard Specifications

Grade Inconel 600 – UNS N06600, Nickel Alloy 600
Specification ASTM B166 UNS N06600, AMS 5665
Flat bar size Thickness: 2 -100mm
Width: 10 to 500mm
Square bar size 4 to 100mm
Round bar size Diameter: 3-~800mm
Hex Bar size 2-100mm A/F
Channel Bar 80 x 40mm to 150 x 75mm section; 5.0 to 6.0mm thickness
Hollow Bar 32mm OD x 16mm ID to 250mm OD x 200mm ID)
Angle bar size 3mm*20mm*20mm~12mm*100mm*100mm
Section 3.0 to 12.0mm thickness
Rectangles Size 33 x 30mm to 295 x 1066mm
Billet Size 1/2″ to 495mm Diameter
Finish Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black
Condition Hardened & tempered, annealed
Technique 600 Inconel Cold Drawn, Hot Rolled, Forged Round Bar, Rod, Cold Rolled
Tolerance H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements
Surface Cold Drawn, Bright, Sand Blasting Finished, Hot Rolled Pickled, Hairline, Polished
Processing Bar cutting to 650mm

 

Inconel 600 Round Bar Weight Chart

Opp width Weight Sectional Area
mm kg/m cm2
16 1.74 2.217
17 1.96 2.49
13 1.15 1.463
19 2.45 3.126
18 2.2 2.806
10 0.68 0.866
8 0.435 0.5542
9 0.551 0.7015
14 1.33 1.697
11 0.823 1.048
15 1.53 1.948
12 0.979 1.247
20 2.72 3.464

 

Heat Treatment Process for Nickel 600 Round Bar

Annealing 1850°F - 2100°F (1010°C - 1150°C)
Recrystallization Anneal 1900°F - 1950°F (1040°C - 1065°C)
Stress Relieving 1600°F - 1800°F (870°C - 980°C

 

Inconel 600 Round Bar Temperature Range

Properties Value
Max Service Temperature Up to 2000°F (1093°C)
Continuous Use Temperature Up to 1500°F (815°C)

 

ASTM B166 Inconel 600 Cold Drawn Round Bar Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

 

ASME SB166 Inconel 600 Round Bars Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.47 g/cm3 1413 °C (2580 °F) 655 MPa, 95000 psi 310 MPa, 45000 psi 45 %
Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry