Monel 400 Flanges

Everything You Need to Know About Monel 400 Flanges
Monel 400 flanges are made from a nickel-copper alloy known for their high strength, excellent corrosion resistance, and ability to maintain performance over a wide temperature range. These flanges are crucial in industries such as oil and gas, chemical processing, and marine applications because they can withstand a variety of corrosive environments, including seawater, acids, and alkalis.
What is the ASTM standard for Monel 400 flanges?
Monel 400 flanges are made of a copper-nickel alloy that offers excellent ductility, strength, and resistance to acid corrosion. Furthermore, the alloy is stable at high temperatures and can be hardened during cold working.


Will Monel 400 alloy flanges rust?
The corrosion resistance of Monel 400 alloy flanges is particularly important in marine environments. They are widely used in marine components, including propeller shafts and fasteners, which are frequently exposed to seawater.
Alloy 400 Flange Mechanical Strength
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Chemical Compatibility of Nickel Alloy 400 Flange
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel 400 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
Density & Melting point of Monel 400 Flanges
| Density | 8.83 g/cm³ |
| Melting point | 1300-1390 ℃ |
Nickel Alloy 400 Flange Pressure Rating
| Temp. °C | Class 150 | Class 300 | Class 400 | Class 600 | Class 900 | Class 1500 | Class 2500 |
|---|---|---|---|---|---|---|---|
| -29~38 | 15.9 | 41.4 | 55.2 | 82.7 | 124.1 | 206.8 | 344.7 |
| 50 | 15.4 | 40.2 | 53.7 | 80.5 | 120.7 | 201.2 | 335.3 |
| 100 | 13.8 | 35.9 | 47.9 | 71.9 | 107.8 | 179.7 | 299.5 |
| 150 | 12.9 | 33.7 | 45.0 | 67.5 | 101.2 | 168.7 | 281.1 |
| 200 | 12.5 | 32.7 | 43.6 | 65.4 | 98.1 | 163.5 | 272.4 |
| 250 | 12.1 | 32.6 | 43.5 | 65.2 | 97.8 | 163.0 | 271.7 |
| 300 | 10.2 | 32.6 | 43.5 | 65.2 | 97.8 | 163.0 | 271.7 |
| 325 | 9.3 | 32.6 | 43.5 | 65.2 | 97.8 | 163.0 | 271.7 |
| 350 | 8.4 | 32.6 | 43.4 | 65.1 | 97.7 | 162.8 | 271.3 |
| 375 | 7.4 | 32.4 | 43.2 | 64.8 | 97.2 | 161.9 | 269.9 |
| 400 | 6.5 | 32.1 | 42.8 | 64.2 | 96.2 | 160.4 | 267.4 |
| 425 | 5.5 | 31.6 | 42.2 | 63.3 | 94.9 | 158.2 | 263.6 |
| 450 | 4.6 | 26.9 | 35.9 | 53.8 | 80.7 | 134.5 | 224.2 |
| 475 | 3.7 | 20.8 | 27.7 | 41.5 | 62.3 | 103.8 | 173.0 |

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, incoloy 825, monel alloy 400, monel k500 and high temperature alloy materials. It specializes in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automobile, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to know the alloy material price consultation or provide customized alloy material solutions, you are welcome to contact us at any time to get a quote at ss@gneesteel.com