The ASTM B564 UNS N04400 90-degree elbow is a piping component made from Monel 400. Monel 400 is a nickel-copper alloy known for its excellent corrosion resistance, especially in seawater, and good mechanical properties and strength over a wide temperature range. Its key properties include: it cannot be hardened by heat treatment but is easily cold worked; it is suitable for marine and chemical processing applications; and its high tensile and yield strengths can be increased by cold working.

What is the composition of Monel 400 alloy?

Monel 400 is primarily a nickel-copper alloy with a typical chemical composition of at least 63% nickel (including cobalt), 28-34% copper, and up to 2.5% iron, 2.0% manganese, 0.5% silicon, 0.3% carbon, and 0.024% sulfur. This composition provides Monel 400 with excellent corrosion resistance in marine environments and various acid and alkaline solutions, making it suitable for use in chemical processing equipment, offshore engineering, and heat exchangers.

Monel 400 Alloy
 

Monel 400 Chemical Composition

Chemical Requirements
Monel 400 Ni C Mn S Si Cu Fe
Max   0.3 2 0.024 0.5 34 2.5
Min 63         28  

 

Monel 400 Mechanical Properties

Mechanical Property Requirements
Monel 400 Ultimate Tensile Yield Strength (0.2% OS) Elong. in 2 in. or 50mm (or 4D), min.,% R/A Hardness
Cold Worked/SR
Min 87 KSi 60 KSi 20B    
Max          
Min 600 MPa 415 MPa      
Max          
Hot Worked/SR
Min 80 KSi 40 KSi 30D    
Max          
Min 552 MPa 276 MPa      
Max          

 

Material Properties and Composition
Alloy: Monel 400, designated UNS N04400.
Composition: Primarily a nickel-copper alloy, with approximately 67% nickel and 31% copper.
Hardenability: It is a solid solution alloy and can only be hardened by cold working, not heat treatment.

 

Key Features and Benefits
Corrosion Resistance: Excellent corrosion resistance in seawater, saltwater, and other environments, as well as in a wide range of acid and alkaline conditions.
Mechanical Strength: High tensile and yield strength, further improved by cold working.
Temperature Range: Maintains strength over a wide temperature range, including subzero and cryogenic temperatures.
Versatility: Excellent performance in a wide range of corrosive environments, making it suitable for a wide range of applications.

 

Common Applications
Marine: Used in pumps, valves, and propeller shafts used in marine applications and offshore structures.
Chemical Processing: Used in plants involving sulfuric, hydrofluoric, and hydrochloric acids, as well as in the production of chlorinated plastics and perchloroethylene.
Petroleum Refining: Used in crude oil distillation columns and transmission pipelines. Power Generation: For boiler feedwater and steam generator piping.

 

Important Considerations
Stagnant Conditions: While performing well in flowing seawater, stagnant conditions may result in crevice corrosion and pitting.
Mechanical Testing: ASTM B564 requires chemical analysis, grain size determination, and mechanical property testing (tensile, yield, elongation).

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.