Apr 01, 2024 Leave a message

ASTM A240 Grade 330 Plate

GNEE Steel is a distinguished exporter, supplier, distributor and manufacturer of ASTM A240 TP330 Plate.We are well known trader of Stainless Steel 330 Plates in China.We producing stainless steel 330 plate & SS 330 Sheet since 1999.We maintain over 800 ton SS 330 Plates in various shape,sizes & coating which makes us one of the largest stockholder 330 SS Plate in China.We are ISO 9001:2008 certified manufacturer of ASTM A240 Grade 330 plate & now we became Distributor of UNS N08330 Sheet & DIN 1.4864 Stainless Steel Plate. We are largest exporter and Supplier of ASTM A240 TP330 Stainless steel Plate in China.We offer 330 stainless steel plate in various sizes at best price.

 

Stainless Steel Sheet MetalStainless Steel Sheet

ASTM A240 SS 330 Plate Specifications

Standard ASTM, ASME, BS, DIN, EN
Material 310S, 310, 309, 309S, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H, 304, 304L,
302, 301, 201, 202, 403, 405, 409, 409L, 410, 410S, 420, 430, 631, 904L, Duplex, etc
Specification Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.

Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt.

Technique Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc.
Surface 2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching
Thickness 0.25-200mm, 0.3mm to 120mm
Width 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm
Length 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm
Package Standard Export Seaworthy Package, or as required.
Value Added Services Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc.
MTC Mill Test Certificate, Available as per EN 10204 3.1

 

ASTM A240 Stainless Steel 330 Plate Chemical Composition

Element Content (%)
Iron, Fe 42
Nickel, Ni 36
Chromium, Cr 19
Manganese, Mn 2
Silicon, Si 1.13
Carbon, C 0.080
Phosphorous, P 0.040
Sulfur, S 0.030

ASTM A240 TP330 Stainless Steel Sheet Physical Properties

Properties Metric Imperial
Density 8 g/cm3 0.289 lb/in³

ASTM A240 SS 330 Plate Mechanical Properties

Properties Metric Imperial
Tensile strength, ultimate 550 MPa 79800 psi
Tensile strength, yield (@0.2%) 260 MPa 37700 psi
Modulus of elasticity 197 GPa 28600 ksi
Poisson's ratio 0.27 – 0.30 0.27 – 0.30
Elongation at break (in 50 mm) 40% 40%

 

330 Stainless Steel Plate Stock

ASTM A240 TP330 Stainless Steel 2B Finish Plate ASTM A240 TP330 Stainless Steel Cold Rolled Plates
ASTM A240 TP330 Stainless Steel 4 Finish Plate ASTM A240 TP330 Stainless Steel 2D Finish Plate
ASTM A240 TP330 Stainless Steel CR Plates ASTM A240 TP330 Stainless Steel 8 Finish Plate
ASTM A240 TP330 Stainless Steel Hot Rolled Plates Stainless Steel ASTM A240 TP330 HR Plates
ASTM A240 TP330 Stainless Steel Plates ASTM A240 TP330 Stainless Steel Chequered Plate
ASTM A240 TP330 Stainless Steel Cut to Size Plate ASTM A240 TP330 Stainless Steel High quality plate

 

Send Inquiry