ASTM A240/ ASME SA 240 Grade 201 Stainless Steel Sheet

GNEE Steel is prominent manufacturer, supplier and exporter of ASTM A240 Stainless Steel 201 Plate. We are Manufacturer of Stainless Steel 201 Plates in China ,we are producing stainless steel 201 plate & SS 201 Sheet from many years.We are ISO 9001 & PED approved Exporter of ASTM A240 TP201 Stainless steel Plate in China.We maintain over 1200 ton 201 stainless steel plate in various shape,sizes & coating which makes us one of the largest stockist of 201 SS Plate in China.

stainless sheetStainless Steel Sheet

 

ASTM A240 SS 201 Plate Specifications

Description ASTM A240 / ASME SA240 Stainless Steel Plates, ASTM A240 Hot Rolled Stainless Steel Plates
Standard ASTM, ASME, BS, DIN, EN
Material 310S, 310, 309, 309S, 316, 316L, 316Ti, 317, 317L, 321, 321H, 347, 347H, 304, 304L,
302, 301, 201, 202, 403, 405, 409, 409L, 410, 410S, 420, 430, 631, 904L, Duplex, etc
Specification Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement.

Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt.

Technique Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc.
Surface 2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching
Thickness 0.25-200mm, 0.3mm to 120mm
Width 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm
Length 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm
Package Standard Export Seaworthy Package, or as required.
Value Added Services Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc.
MTC Mill Test Certificate, Available as per EN 10204 3.1


SS 201 Plate Equivalent grades

JIS G4304 ASTM UNS KS EN10095 AS CNS
SUS201 201 S20100 STS201 1.4372 201-2 201


ASTM A240 Stainless Steel 201 Plate Chemical Composition

Grade C Mn Si P S Cr Ni N
SS 201 0.15 max 5.5 – 7.5 100 max 0.06 max 0.03 max 16.00-18.00 0.3 – 0.5 –


ASTM A240 TP201 Stainless Steel Sheet Physical Properties

Properties

Metric

Imperial

Density

7.86 g/cm3

0.284 lb/in³

 