Nov 08, 2025 Leave a message

ASME SB407 UNS N08811 Nickel-iron-chromium Alloy High-temperature Industrial Piping

 
ASME SB407 UNS N08811 Nickel-iron-chromium alloy high-temperature industrial piping
 

Gnee Steel

 

ASME SB407 UNS N08811 Nickel-iron-chromium alloy high-temperature industrial piping

ASME SB407 UNS N08811 tubing is a high-performance nickel-iron-chromium alloy renowned for its excellent high-temperature and corrosion resistance. Its key characteristics include maintaining high strength at high temperatures (up to approximately 1093°C), excellent resistance to oxidation, carburization, and stress corrosion cracking, and compliance with stringent quality standards. This tubing is widely used in demanding industrial applications such as petrochemical processing, heat exchangers, and steam generators.

GH4169 High-temperature alloy pipes for deep-sea oil and gas environments

Gnee Steel

 

What is SB 407 material?

What is ASTM B407 pipe? ASTM B407 alloy is composed of nickel, iron, and chromium. This specification is generally applied to seamless pipe and covers Incoloy 800 and Incoloy H/HT alloys.

 SB 407 material

Chemical Requirements for UNS N08811 Pipe

Element

Nickel

Chromium

Iron

Manganese, max

Carbon

Copper

Silicon

Sulfur, max

Aluminum

Titanium

Composition Limits, %

30 min – 35 max

19 min – 23 max

36.5 min

1.5

–

0.75

1

0.015

0.15 min – 0.60max

0.15 min – 0.60max

 

Mechanical Properties of UNS N08811 Tube

Alloy

Condition (Temper)

Tensile Strength

Yield Strength (0.2 % offset, min)

Elongation in 2 in. or 50 mm (0.8 in.), min

UNS N08811

hot - finished annealed or cold - worked annealed

65,000 (450) psi (MPa)

25,000 (170) psi (MPa)

30

 

Pipe Schedules

Normal Pipe Size

Outside Diameter

Schedule No. 5

Schedule No. 10

Schedule No. 40

Schedule No. 80

Inches

1/4

0.54

--

0.065

0.088

--

3/8

0.675

--

0.065

0.091

0.126

1/2

0.84

0.065

0.083

0.109

0.147

3/4

1.05

0.065

0.083

0.113

0.154

1

1.315

0.065

0.109

0.133

0.179

1 1/4

1.66

0.065

0.109

0.14

0.191

1 1/2

1.9

0.065

0.109

0.145

0.2

2

2.375

0.065

0.109

0.154

0.218

2 1/2

2.875

0.083

0.12

0.203

0.276

3

3.5

0.083

0.12

0.216

0.3

3 1/2

4

0.083

0.12

0.226

0.318

4

4.5

0.083

0.12

0.237

0.337

5

5.563

--

--

0.258

--

6

6.625

--

--

0.28

--

Millimetres

6.35

13.72

--

1.65

2.24

--

9.52

17.14

--

1.65

2.31

3.2

12.7

21.34

1.65

2.11

2.77

3.73

19.05

26.67

1.65

2.11

2.87

3.91

25.4

33.4

1.65

2.77

3.38

4.55

31.8

42.16

1.65

2.77

3.56

4.85

38.1

48.26

1.65

2.77

3.68

5.08

50.8

60.32

1.65

2.77

3.91

5.54

63.5

73.02

2.11

3.05

5.16

7.04

76.2

88.9

2.11

3.05

5.49

7.62

88.9

101.6

2.11

3.05

5.74

8.08

101.6

114.3

2.11

3.05

6.02

8.56

127.0

141.3

--

--

6.55

--

152.4

168.28

--

--

7.11

--

 

Advantages of ASME SB407 UNS N08811

1. Excellent High-Temperature Resistance

Maintains stable mechanical properties at high temperatures (e.g., 650–1093°C), resisting deformation/cracking under pressure and ensuring pipeline stability.

2. Strong Corrosion Resistance

Resistant to oxidizing acids (such as nitric acid), sulfur-containing media, and stress corrosion.

Reduces leakage risk, suitable for high-temperature corrosive environments such as chemical and petrochemical industries.

3. Superior Structure and Quality Assurance

Seamless Construction: Uniform wall thickness, no weak welds, ideal for high-pressure/high-purity fluid transportation.

Compliant with ASME SB407 Standard: Rigorous testing (chemical, mechanical, and non-destructive testing) ensures reliable quality.

4. Good Machinability

Easy to Form: Can be cold-worked/hot-worked into various shapes (straight/bends) to meet different design requirements. Weld-Friendly: Weld properties match the base material properties, reducing installation/maintenance costs.

 

Why Choose Gnee Nickel Alloy (Supplier Example)?

✅ Large stock of Incoloy 800/800H/800HT alloy tubes/bars/plates/fittings, fast shipping.

✅ Factory direct sales, highly competitive prices, excellent value for money.

✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical properties certificate.

✅ Value-added services: slitting, cutting, polishing, surface treatment.

✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.

Email: ss@gneesteel.com

Gnee Steel

 

About Gnee Steel

Gnee Steel is a professional manufacturer of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions according to customer needs. For alloy material price inquiries or to request customized alloy material solutions, please feel free to contact us at ss@gneesteel.com for a quote.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry