Jan 12, 2024 Leave a message

American Standard UNS N08811 Chemical Composition, Mechanical Properties And Uses

American standard UNS N08811 chemical composition, mechanical properties and uses

 

UNS N08811 is a fully austenitic low-carbon nickel-iron-chromium alloy in the same series as Incoloy 800. The cobalt content in this alloy can be strictly controlled below 0.01%.

UNS N08811 is resistant to many corrosive media. Its high nickel content makes it very resistant to stress corrosion cracking in aqueous corrosive conditions. The high chromium content gives it better resistance to pitting and crevice corrosion cracking. This alloy has good corrosion resistance to nitric acid and organic acids, but has limited corrosion resistance in sulfuric acid and hydrochloric acid. In addition to the possibility of pitting corrosion in halides, it has good corrosion resistance in oxidizing and non-oxidizing salts. It also has good corrosion resistance in water, steam and mixtures of steam, air and carbon dioxide.

American standard UNS N08811 chemical composition, mechanical properties and uses

American standard UNS N08811 chemical composition, mechanical properties and uses

UNS N08811 has the following properties

●Excellent corrosion resistance in extremely high temperature aqueous media up to 500°C

●Very good resistance to stress corrosion

●Very good processability

UNS N08811 uses:

●Nitric acid condenser - resistant to nitric acid corrosion

●Steam heating tube - good mechanical properties

●Heating element tube - good mechanical properties

●For applications in environments up to 500°C, the alloy is supplied in the annealed state.

 