Monel 400 N04400 2.4360 Alloy Sheet
Product Introduction
Monel Alloy 400 is a nickel-copper (about 67% Ni – 23% Cu) solid solution strengthened alloy. The alloy is characterized by moderate strength, good weldability, good general corrosion resistance and toughness. It is useful at temperatures up to 1000°F (538°C). Alloy 400 has excellent resistance to rapidly flowing brackish or seawater where cavitation and erosion resistance is necessary. It is particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated. Alloy 400 is slightly magnetic at room temperature.
ASTM Specifications
| Pipe Smls | Pipe Welded | Tube Smls | Sheet / Plate | Bar | Forging | Fitting |
| B165 | B725 | B163 | B127 | B164 | B564 | B366 |
Chemical Composition
| Trade Name |
ASTM/AISI Alloy type |
UNS | %Cu | %Fe | %Mn | %Si | %Ni |
| Monel 400 | B 127, B 164 | N04400 | 28–34 | 2.5 max | 2.0 max | 0.5 max | 63 min |
Mechanical Properties Minimum Room Temperature Tensile Data
| Product Form | Condition | Tensile (ksi) | .2% Yield (ksi) | Elongation (%) | Hardness (HRB) |
| Rod & Bar | Annealed | 75-90 | 25-50 | 60-35 | 60-80 |
| Rod & Bar | Cold-Drawn Stress Relieved | 84-120 | 55-100 | 40-22 | 85-20 HRC |
| Plate | Annealed | 70-85 | 28-50 | 50-35 | 60-76 |
| Sheet | Annealed | 70-85 | 30-45 | 45-35 | 65-80 |
| Tube & Pipe Seamless | Annealed | 70-85 | 25-45 | 50-35 | 75 max* |