404 405 Monel Piping
video

404 405 Monel Piping

Monel R-405 alloy (UNS N04405) increases the sulfur content in the Monel 400 component to enhance the machining performance and becomes a free-cutting Monel alloy.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 404 405 monel piping in China. If you're going to wholesale high quality 404 405 monel piping made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

404 405 Monel Piping

Monel R-405 alloy (UNS N04405) increases the sulfur content in the Monel 400 component to enhance the machining performance and becomes a free-cutting Monel alloy.

Element
Composition limits, %
nickel
63.0min
copper
28min~34max
iron
2.5max
manganese
2.0max
carbon
0.3max
silicon
0.5max
sulfur
0.025min-0.060max

Hot Tags: 404 405 monel piping, China 404 405 monel piping suppliers, formable alloy, alloy application, alloy technical data, alloy experience, alloy insurance, nickel copper alloy