Monel 450 Alloy Plate
video

Monel 450 Alloy Plate

Monel 450 is a nickel-copper alloy renowned for its excellent corrosion resistance and high strength. It is a precipitation-hardenable alloy with additions of aluminum and titanium, which impart enhanced mechanical properties and corrosion resistance. Monel 450 alloy plate finds widespread applications across industries where high strength and corrosion resistance are essential.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 450 alloy plate in China. If you're going to wholesale high quality monel 450 alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Introduction to Monel 450 Alloy Plate:

Monel 450 is a nickel-copper alloy renowned for its excellent corrosion resistance and high strength. It is a precipitation-hardenable alloy with additions of aluminum and titanium, which impart enhanced mechanical properties and corrosion resistance. Monel 450 alloy plate finds widespread applications across industries where high strength and corrosion resistance are essential.

4 140

Key Features:


High Strength: Precipitation hardening gives Monel 450 its remarkable strength, which is one of its primary characteristics. This qualifies it for use in structural elements and equipment that is subjected to high mechanical loads and stress, such as chemical processing equipment, maritime fittings, and aviation components.
Precipitation Hardenability: Heat treatment can fortify Monel 450 since it is a precipitation-hardenable alloy. This makes it a flexible material for a range of technical applications and enables customizable mechanical characteristics to satisfy individual application needs.

4 259

 

Applications:

 

Aerospace: Monel 450 alloy plate finds extensive use in aerospace applications, including aircraft components, structural parts, and landing gear components. Its high strength-to-weight ratio and corrosion resistance make it suitable for critical aerospace components.

Marine Engineering: In marine engineering applications, Monel 450 is utilized in seawater piping systems, marine fittings, and propeller shafts. Its corrosion resistance and mechanical properties make it ideal for components exposed to harsh marine environments.

 

Specifications:

 

Specification Description
Thickness 0.1 mm - 10 mm
Width 100 mm - 2000 mm
Length Customized
Surface Finish Cold Rolled, Hot Rolled, Acid Pickled, Bright Surface
Material Monel 450 Alloy
Strength ≥ 550 MPa
Tensile Strength ≥ 1100 MPa
Yield Strength ≥ 480 MPa
Density 8.80 g/cm³
Melting Point 1300-1350°C
Corrosion Resistance Excellent resistance to seawater, acids, alkalis, etc.
Typical Applications Aerospace, Marine Engineering, Chemical Processing
Manufacturing Standards ASTM B127, ASME SB127

 

In summary, Monel 450 alloy plate offers exceptional corrosion resistance, high strength, and precipitation hardenability, making it a preferred choice for critical applications across aerospace, marine engineering, and chemical processing industries.

 

FAQ:

Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.

 

Q: Can you provide us sample, is it free or need to pay?
A: If you don't need to print your logo or other artwork on the products, we will not charge any cost, just tell us your freight collect account like Fedex, DHL, TNT. If you don't have, we need to charge Express fee properly.

 

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.

 

Hot Tags: monel 450 alloy plate, China monel 450 alloy plate suppliers, brazability alloy, alloy surplus, alloy blends, alloy weakening, alloy disadvantage, alloy shortage

Send Inquiry

whatsapp

Phone

E-mail

Inquiry