MONEL 400 Seamless Pipe Specifications:
Sizes: ASTM, ASME and API
Standards:
ASTM B165/ ASME SB165
Sizes: 1/8″NB to 30″NB IN
Expertise: Large Diameter Sizes
Specifications: SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Shapes: Round, Hydraulic, etc.
Types: Seamless/Processed
Lengths: Single Random, Double Random and Cut Lengths.
Ends: Plain, Bevel, Threaded
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel uns no4400 n04405 corrosion resistant tubing in China. If you're going to wholesale high quality monel uns no4400 n04405 corrosion resistant tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Uns No4400 N04405 Tubing Equivalent grade

monel uns no4400 n04405 Tubing video

GNEE STEEL GROUP supplies Uns No4400 N04405 Tubing for you

 

GNEE STEEL GROUP supplies alloy 400 Tubing

 

UNS N04400

Other common names: Alloy 400

W.Nr.2.4360, 2.4361

ASTM: B164, B564, B127, B165, B725, B730

ASME: SB164, SB564, SB127, SB165, SB725, SB730

QQ-N-281

Mil-T-1368

EN10204 3.1

Form

Standard

Metal Type

UNS N04400

Bar

ASTM B164 QQ-N-281 Din 17750

Wire

 

Sheet

ASTM B127 QQ-N-281

Plate

ASTM B127 QQ-N-281

Pipe

ASTM B165

Tube

ASTM B165

Fitting

 

Forging

ASTM B564

Weld Wire

FM 60/ ERNiCu-7/ 17753

Weld Electrode

FM 190 ENiCu-7

Din

2.4360

GNEE STEEL GROUP supplies UNS N04405 Material Alloy Tubing

UNS N04405

W.Nr.2.4363

ASTM B164

ASME SB164

QQ-N-281

Form

Standard

Metal Type

UNS N04405

Bar

ASTM B164 QQ-N-281

Wire

 

Sheet

ASTM B127 QQ-N-281

Plate

ASTM B127 QQ-N-281

Fitting

 

Forging

ASTM B564

Weld Wire

 

Weld Electrode

FM 190/ ENiCu-7

 

Uns No4400 N04405 Tubing chemical composition

monel 400 Tubing chemical composition

Element Content (%)
Nickel, Ni 63-70
Copper, Cu 28-34
Iron, Fe 2.5
Manganese, Mn 2
Silicon, Si 0.5
Carbon, C 0.3
Sulfur, S 0.024

monel 405 Tubing chemical composition

Element Content (%)
Nickel+Cobalt, Ni+Co 63
Copper, Cu 28-34
Iron, Fe 2.5
Manganese, Mn 2
Silicon, Si 0.5
Carbon, C 0.3
Sulfur, S 0.025-0.06

uns no4400 n04405 Tubing

uns no4400 n04405 seamless Tubing suppliersuns no4400 n04405 ss Tubing price

Monel 400 alloy (UNS N04400 or MCu-28-1.5-1.8 or Ni68Cu28Fe) is a nickel-based alloy material. It has excellent corrosion resistance in seawater, chemical solvents, ammonia sulfur chloride, hydrogen chloride, and acidic media such as sulfuric acid, hydrofluoric acid, hydrochloric acid, phosphoric acid, and organic acids, as well as alkaline media, salts, and molten salts. In addition, it has excellent mechanical properties, can be used in a wide range from low temperature to high temperature, and has good welding performance and medium to high strength.
Monel R405 is a nickel-copper alloy also known as UNS N04405, part of the Monel family of high-temperature alloys. Monel 405 is typically available in rod, rod and wire forms and offers enhanced processability due to its higher sulfur content. In addition, this high-temperature alloy has excellent corrosion resistance, high strength and good weldability.

GNEE Group Factory Environment

Monel Uns No4400 corrosion resistant Tubing

Monel Uns No4400 N04405 corrosion resistant Tubing

Uns No4400 N04405 Tubing material & size

Uns No4400 N04405 Tubing material & size

Uns No4400 N04405 Tubing

Uns No4400 N04405 Tubing

 

customer visit

customer visit

Uns No4400 N04405 Tubing

 

FAQ

Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: About the product price of uns no4400 n04405 steel Tubing?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

contact us

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

Hot Tags: Monel Uns No4400 N04405 corrosion resistant Tubing, China Monel Uns No4400 N04405 corrosion resistant Tubing suppliers, alloy invoice, alloy development, alloy plate, alloy forging, alloy receipt, alloy cost

Send Inquiry

whatsapp

Phone

E-mail

Inquiry