ASTM B165 Monel 400 Corrosion-resistant Nickel Pipe For Seawater
Standards: Conforms to ASTM B165 and UNS N04400.
Condition: Typically supplied in the annealed or stress-relieved condition.
Marking: The pipe is marked with the standard, grade, outer diameter, thickness, length, and batch number.
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b165 monel 400 corrosion-resistant nickel pipe for seawater in China. If you're going to wholesale high quality astm b165 monel 400 corrosion-resistant nickel pipe for seawater made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater description

GNEE ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater
ASTM B165 Monel 400 pipe is an ideal choice for seawater applications due to its excellent corrosion resistance in saline solutions and high mechanical strength at both high and low temperatures. Key properties include its composition (nickel-copper alloy), its resistance to various acids (after degassing), and its use in components such as pumps, valves, and heat exchangers in the marine, chemical, and petroleum industries. However, it's important to note its higher cost and its tendency to harden during processing.
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Specification
Monel 400 Pipe Specification
| Specifications and Dimensions | ASTM B 165 ASME SB 165 / ASTM B 725 ASME SB 725 |
|---|---|
| Size in Inches | 15- 150 |
| OD | 6.35- 254 mm |
| Most popular types | Seamless / ERW / Welded / Fabricated |
| Forms / Shapes | Round, Square, Hollow |
| Pipe End Type Abbreviations | Plain End, Beveled End, PBE, BBE, TOE, BE, TBE, BOE, BSE, BLE, POE, BOE, Treaded |
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Chemical Composition
Monel 400 corrosion-resistant nickel alloy pipe for seawater Mechanical Properties:
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Monel 400 corrosion-resistant nickel alloy pipe for seawater Equivalent Material:
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel 400 | 2.4360 | N04400 | NW 4400 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
Monel 400 corrosion-resistant nickel alloy pipe for seawater Physical Properties:
| PROPERTIES | METRIC | IMPERIAL |
|---|---|---|
| Density | 8.8 gm/cm3 | 0.318 lb/in3 |
Schedule Chart Of ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater
Monel 400 Pipe Schedule and Wall Thickness
|
NOMINAL |
O.D. INCHES |
10S |
10 |
40S & STD |
40 |
80S & E.H. |
80 |
160 |
|---|---|---|---|---|---|---|---|---|
|
1/8 |
.405 |
.049 |
.049 |
.068 |
.068 |
.095 |
.095 |
|
|
1/4 |
.540 |
.065 |
.065 |
.088 |
.088 |
.119 |
.119 |
|
|
3/8 |
.675 |
.065 |
.065 |
.091 |
.091 |
.126 |
.126 |
|
|
1/2 |
.840 |
.083 |
.083 |
.109 |
.109 |
.147 |
.147 |
.187 |
|
3/4 |
1.050 |
.083 |
.083 |
.113 |
.113 |
.154 |
.154 |
.218 |
|
1 |
1.315 |
.109 |
.109 |
.133 |
.133 |
.179 |
.179 |
.250 |
|
1 1/4 |
1.660 |
.109 |
.109 |
.140 |
.140 |
.191 |
.191 |
.250 |
|
1 1/2 |
1.900 |
.109 |
.109 |
.145 |
.145 |
.200 |
.200 |
.281 |
|
2 |
2.375 |
.109 |
.109 |
.154 |
.154 |
.218 |
.218 |
.343 |
|
2 1/2 |
2.875 |
.120 |
.120 |
.203 |
.203 |
.276 |
.276 |
.375 |
|
3 |
3.500 |
.120 |
.120 |
.216 |
.216 |
.300 |
.300 |
.437 |
|
3 1/2 |
4.000 |
.120 |
.120 |
.226 |
.226 |
.318 |
.318 |
|
|
4 |
4.500 |
.120 |
.120 |
.237 |
.237 |
.337 |
.337 |
.531 |
|
4 1/2 |
5.000 |
|
|
.247 |
|
.355 |
|
|
|
5 |
5.563 |
.134 |
.134 |
.258 |
.258 |
.375 |
.375 |
.625 |
|
6 |
6.625 |
.134 |
.134 |
.280 |
.280 |
.432 |
.432 |
.718 |
|
7 |
7.625 |
|
|
.301 |
|
.500 |
|
|
|
8 |
8.625 |
.148 |
.148 |
.322 |
.322 |
.500 |
.500 |
.906 |
|
9 |
9.625 |
|
|
.342 |
|
.500 |
|
|
|
10 |
10.750 |
.165 |
.165 |
.365 |
.365 |
.500 |
.593 |
1.125 |
|
11 |
11.750 |
|
|
.375 |
|
.500 |
|
|
|
12 |
12.750 |
.180 |
.180 |
.375 |
.406 |
.500 |
.687 |
1.312 |
|
14 |
14.000 |
.188 |
.250 |
.375 |
.437 |
.500 |
.750 |
1.406 |
|
16 |
16.000 |
.188 |
.250 |
.375 |
.500 |
.500 |
.843 |
1.593 |
|
18 |
18.000 |
.188 |
.250 |
.375 |
.562 |
.500 |
.937 |
1.781 |
Monel 400 UNS N04400 Pipe Pressure Rating
| ALLOY 400 PIPE O.D. (IN.) |
WALL THICKNESS OF PIPE (INCHES) | |||||||
|---|---|---|---|---|---|---|---|---|
| .028 | .035 | .049 | .065 | .083 | .095 | .109 | .120 | |
| WORKING PRESSURE (PSIG) | ||||||||
| 1/8 | 7900 | 10100 | ||||||
| 1/4 | 3700 | 4800 | 7000 | 9500 | ||||
| 5/16 | 3700 | 5400 | 7300 | |||||
| 3/8 | 3100 | 4400 | 6100 | |||||
| 1/2 | 2300 | 3200 | 4400 | |||||
| 3/4 | 2200 | 3000 | 4000 | 4600 | ||||
| 1 | 2200 | 2900 | 3400 | 3900 | 4300 | |||
Application of ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Applications
Marine: Widely used in marine equipment, pumps, valves, and piping systems in contact with seawater.
Chemical and Petroleum: Used in chemical reactors, heat exchangers, and piping in the chemical processing, oil, and gas industries.
Other: Used in desalination equipment, aerospace components, and other applications requiring high performance in high-temperature and corrosive environments.
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater process
Testing of ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Pipe
Packing of ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater
ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Packaging
Standard Packaging Methods:
Steel Strapping:
Pipe with an outer diameter of 3 inches or less is typically strapped together with polypropylene film to prevent rust during ocean shipping, and then secured with steel strapping.
Wooden Cases/Crates:
Pipe is typically packaged in wooden cases or crates for protection during transportation, especially long or large diameter pipe.
Seaworthy Export Packaging:
Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipe during transportation.
Typo-Proof Packaging:
Export crates are designed to prevent rain, seawater, and other external water from penetrating during transportation.
About Gnee Steel

Gnee Steel is a supplier of Monel 400 Nickel-Copper Alloy. Our product offerings include seamless tubes (sizes: 4-219 mm, thicknesses: 0.5-20 mm); welded tubes (sizes: 5.0-1219.2 mm, thicknesses: 0.5-20 mm); plate (sizes: 0.1-100 mm, widths: 10-2500 mm); strip; alloy round bar (sizes: 3-800 mm, diameters: 2-100 mm, widths: 10-500 mm); hexagonal bar (sizes: 2-100 mm); wire rod; and extruded sections. We partner with steel mills to provide our customers with Alloy 400 that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS.
Gnee Steel stocks and sells Monel 400 Nickel-Copper Alloy, pipes, tubes, plates, strip, sheets, round bars, flat bars, forging billets, hexagons, wire rod, and extruded shapes. Feel free to contact us for a quote at ss@gneesteel.com
Hot Tags: ASTM B165 Monel 400 Corrosion-resistant Nickel Pipe For Seawater, China ASTM B165 Monel 400 Corrosion-resistant Nickel Pipe For Seawater suppliers, alloy product catalogue, alloy business, Monel 500, alloy characteristics, alloy msds, alloy annealing
You Might Also Like
Send Inquiry