Monel Alloy K500 Pipe Fittings
video

Monel Alloy K500 Pipe Fittings

Monel K500 Pipe Fittings are made from a nickel-copper alloy with excellent corrosion resistance and high strength. These pipe fittings are often used in marine, industrial & chemical processing applications due to their ability to resist saltwater, sulfuric acid, hydrochloric acid, alkalis & other corrosive chemicals.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy k500 pipe fittings in China. If you're going to wholesale high quality monel alloy k500 pipe fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Product Introduction

 

Monel K500 Pipe Fittings are alloy pipe fittings used in high-temperature and pressure applications. These fittings are made from copper, nickel, and iron alloy and feature corrosion resistance and high strength at elevated temperatures. K500 Pipe Fittings provide excellent resistance to pitting, stress-corrosion cracking, erosion-corrosion, and erosive wear. These fittings have excellent ductility and toughness. Monel K500 Pipe Fittings come in various shapes, sizes, and styles. They include threaded fittings such as 90° elbows, 45° elbows, tees, crosses, couplings, end caps, and plugs. There are also butt weld fittings such as short-radius elbows, long-radius elbows, concentric reducers, eccentric reducers, and caps. There are socket-welded fittings like reducing tee's, socket-welded elbows, socket welded cross' etc., available in this material grade. All these components have different wall thicknesses based on the project needs ranging from sch10 to sch160.

 

Monel K500 Reducer Pipe Fittings are used in many industries because they are ideal for applications that require high strength and corrosion resistance. They are commonly used in power plants due to their ability to withstand extreme temperatures and pressures. They are also great for chemical processing applications where materials must resist strong acids or other corrosive agents. In addition, they can be found in the petrochemical industry, where highly corrosive environments make them an ideal choice for pipe fittings. Monel 400 Pipe Fittings, Monel K500 Round Bars and many more grades are also available.

 

The benefits of Monel Grade K500 Pipe Fittings include excellent corrosion resistance in both acidic and alkaline environments at elevated temperatures, good elasticity, low magnetic permeability, good tensile strength, excellent fatigue strength, excellent welding characteristics, good machinability, non-magnetic properties, oxidation resistance at high temperatures, excellent thermal stability, non-sparking characteristics, superior cold formability, low coefficient of thermal expansion, low electrical resistivity and exceptional dimensional stability over a wide range of temperatures. It is also easier to machine than most stainless steel, making it an ideal choice for intricate designs. Different types of products are available, such as Inconel X750 Forgings, Hastelloy B3 Flanges etc.

 

20240712165409

 

Monel Alloy Butt weld Pipe Fittings offer several advantages over other materials, including excellent corrosion resistance in acidic and alkaline environments at elevated temperatures and good tensile strength and fatigue strength. It has superior cold formability, non-magnetic properties, oxidation resistance at high temperatures, excellent thermal stability,non-sparking characteristics, low electrical resistivity, dimensional stability over a wide range of temperatures, good machinability, and welding characteristics. These features make it the perfect solution for many industrial applications requiring robust materials and superior performance capabilities.

 

What is the difference between Monel K500 Pipe fittings and 400?

Monel K500 and Monel 400 are nickel-copper alloys that offer excellent corrosion resistance in various environments. The primary difference between the two is the addition of aluminum and titanium to Monel K500, which enhances its strength & hardness. Monel K500 suits high-stress applications such as pump and valve components and marine propeller shafts. Monel 400 is still widely used in various industries, but it's typically preferred for less demanding applications where its superior corrosion resistance is the primary factor.

 

Monel Alloy K500 Butt weld Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size Seamless 1/2" - 10" , Welded 1/2" - 48"

Type (Seamless & 100% X-Ray Welded, Fabricated)

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Monel K500 Pipe Fittings UNS (N05500), DIN (2.4375)

 

monel k500

 

Hot Tags: monel alloy k500 pipe fittings, China monel alloy k500 pipe fittings suppliers, 502 2 4360 Monel Alloy Pipe And Tube, alloy financing, alloy powder, alloy market, alloy marketing, alloy specifications