Monel R405 Alloy Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel r405 alloy pipe in China. If you're going to wholesale high quality monel r405 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel R405 Alloy Pipe
Product Introduction
Monel R405 (Alloy 405, UNS N04405) Pipe is a nickel-copper alloy that has a content of cobalt and molybdenum. It has increased sulfur content than Monel 400, thus enhancing machinability into a free-cutting Monel alloy. Like Monel 400, alloy R405 is resistant to seawater and steam at high temperatures, as well as salt, and caustic solutions alkalis. It is also resistant to sulfuric acids and performs well in subzero temperatures.
Monel 405 (Alloy 405, UNS N04405) Tube Specification
Main Specification
|
Density |
8.80g/cm3 |
|
Specific heat |
427 J/kg-°K (20℃) |
|
Modulus of Elasticity |
26 000 ksi |
|
Thermal Conductivity |
21.8 W/mK |
|
Melting range |
1300-1350℃ |
Mechanical Properties
|
Condition |
Tensile (ksi) |
.2% Yield (ksi) |
Elongation % |
Hardness Brinell (3000 kg) |
Hardness Rockwell B |
|
Annealed |
70-85 |
25-40 |
50-35 |
110-140 |
60-76 |
|
Hot-Finished |
75-90 |
35-60 |
45-30 |
130-170 |
72-86 |
|
Cold-Drawn As-Drawn |
85-115 |
50-105 |
35-15 |
160-245 |
85-23C |
Chemical Composition
|
C |
Mn |
S |
Si |
Cr |
Ni |
Mo |
Co |
Ti |
Al |
Fe |
B |
|
0.05-0.12 |
0.10 Max |
0.015 max |
0.50 max |
18.0-20.0 |
Bal. |
9.0-10.5 |
10.0-12.0 |
3.0-3.3 |
1.4-1.6 |
5.0 max |
0.003-0.010 |
Alloy 405 Pipe Applications
- Meter and valve parts
- Screw machine products
- Sulfuric acid plants
- Heat exchangers
- Production
- Crude oil transfer piping
- Propeller and pump shafts
Packaging&Shipping