ASME SB163 Monel 400 Nickel Steel Seamless Pipe For Chemical Industry
video

ASME SB163 Monel 400 Nickel Steel Seamless Pipe For Chemical Industry

Alloy Name: Monel 400
UNS: N04400, W.Nr.2.4360
Forms: Plate, sheet, strip, seamless/welded pipe‑tube, bar, forging, fitting, flange
Matrix type: Solid‑solution nickel‑copper alloy, hardenable only by cold‑work
Key features: Excellent seawater & hydrofluoric acid resistance, good low‑temp toughness
Applicable standards: ASTM B127, B164, B165, B725, B730, B366
Delivery condition: Annealed / cold‑drawn & stress‑relieved
Mandatory inspection: PMI, UT / MT, dimensional verification
Typical industries: Marine, desalination, chemical‑HF equipment, heat‑exchanger, oil‑gas
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of asme sb163 monel 400 nickel steel seamless pipe for chemical industry in China. If you're going to wholesale high quality asme sb163 monel 400 nickel steel seamless pipe for chemical industry made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASME SB163 Monel 400 Nickel Alloy Steel Pipe for Chemical Industry description

ASME SB163 Monel 400 Nickel Alloy Steel Seamless Pipe for Chemical Industry

GNEE ASME SB163 Monel 400 Nickel Alloy Steel Seamless Pipe for Chemical Industry

 

ASME SB163 Monel 400 seamless pipe is a nickel-copper alloy that offers excellent corrosion resistance in a wide range of chemical applications, including hydrochloric, hydrofluoric, and sulfuric acids, as well as seawater and alkaline solutions. It is a strong, durable material with good mechanical properties at both subzero temperatures and elevated temperatures (up to approximately 1020°F or 540°C). The pipe is hardened by cold working and cannot be heat treated to increase its strength.

Contact now

ASME SB163 N04400 Pipe for Chemical Industry Specification

 

 

ASTM B163 Monel 400 Seamless Tubes Specification

 

 

ASTM B163 / ASME SB163 / ASTM B165 / ASME SB165 / ASTM B725 / ASME SB725 / UNS N04400

 

 

ASTM B163 Monel 400 Seamless Tubes Grades

 

 

Monel 400 / MONEL 401 MONEL R-405 / MONEL 404 / MONEL K500 / UNS NO4400

 

 

ASTM B163 Monel 400 Seamless Tubes Type

 

 

to Rolled / Cold Drawn / Welded / ERW

 

 

ASTM B163 Monel 400 Seamless Tubes Outer Diameter Size

 

 

Seamless - 1/4" NB to 6" NB (Nominal Bore Size)
Welded / ERW- 1" NB to 16" NB (Nominal Bore Size)

 

 

ASTM B163 Monel 400 Seamless Tubes Wall Thickness

 

 

Schedule 10 to Schedule 160

 

 

ASTM B163 Monel 400 Seamless Tubes Length

 

 

5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.

 

 

ASTM B163 Monel 400 Seamless Tubes Ends

 

 

Plain Ends / Beveled Ends

 

 

ASTM B163 Monel 400 Seamless Tubes Delivery Conditions

 

 

As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered

 

 

ASTM B163 Monel 400 Seamless Tubes Coating

 

 

Electropolish, Mechanical Polish, Satin Finish, Passivated

 

 

ASTM B163 Monel 400 Seamless Tubes Other Testing

 

 

NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc.

 

 

ASTM B163 Monel 400 Seamless Tubes Dimension

 

 

All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME

 

 

Monel 400 Seamless Tubes Value Added Services

 

 

Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment

 

 

ASTM B163 Monel 400 Seamless Tubes Packaging

 

 

Loose / Bundle / Wooden Pallet / Wooden Box / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector

 

Monel 400 Steel Seamless Pipe for Chemical Industry Chemical Composition

 

Chemical Compatibility Chart of Monel WERKSTOFF NR. 2.4360 Tubing

Grade C Mn Si S Cu Fe Ni
Monel 400 0.30 max 2.00 max 0.50 max 0.024 max 28.00 – 34.00 2.50 max 63.00 min

 

Mechanical Analysis of Monel grade 400 Tube

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel 400 8.8 g/cm3 1350 °C (2460 °F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

 

Schedule Chart Of ASME SB163 Monel 400 Seamless Pipe for Chemical Industry

 

 

Wall Thickness Monel 400 Tube Sizes ( O.D.)
.010 1/16" , 1/8" , 3/16"
.020 1/16" , 1/8" , 3/16" , 1/4" , 5/16" , 3/8"
.012 1/8"
.016 1/8" , 3/16"
.028 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 3/4" , 1" , 1 1/2" , 2"
.035 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 7/16" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.049 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/8" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.065 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 3/4" , 2" , 2 1/2" , 3"
.083 1/4" , 3/8" , 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 7/8" , 2" , 2 1/2" ,3"
.095 1/2" , 5/8" , 1" , 1 1/4" , 1 1/2" , 2"
.109 1/2" , 3/4" , 1" , 1 1/4" , 1 1/2" , 2"
.120 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 2" , 2 1/4" , 2 1/2" , 3"
.125 3/4" , 1" , 1 1/4" , 1 1/2" , 2" , 3" , 3 1/4"
.134 1"
.250 3"
.375 3 1/2"

 

Application of Monel 400 Steel Seamless Pipe for Chemical Industry

 

  • Engineering
    Gnee Steel 
    Engineering
  • Ship Building
    Gnee Steel
    Ship Building
  • Bridges
    Gnee Steel
    Bridges
  • Petrochemical industry
    Gnee Steel
    Petrochemical industry

ASTM B165 Monel 400 corrosion-resistant nickel alloy pipe for seawater Applications
Marine: Widely used in marine equipment, pumps, valves, and piping systems in contact with seawater.
Chemical and Petroleum: Used in chemical reactors, heat exchangers, and piping in the chemical processing, oil, and gas industries.
Other: Used in desalination equipment, aerospace components, and other applications requiring high performance in high-temperature and corrosive environments.

 

ASME SB163 Monel 400 Ss Pipe for Chemical Industry process

  • Annealing process
    Gnee Steel
    Annealing process
  • Hot rolling process
    Gnee Steel
    Hot rolling process
  • Cold drawing process
    Gnee Steel
    Cold drawing process
  • ​​Solution + aging process
    Gnee Steel
    Solution + aging process

 

Testing of ASME SB163 Monel 400 round Pipe for Chemical Industry

 

  • product-275-198
    Gnee Steel
    Expansion test
  • product-276-199
    Gnee Steel
    Dimensional testing
  • product-274-198
    Gnee Steel
    Hardness Test
  • product-274-197
    Gnee Steel
    Nondestructive Testing

 

Packing of ASME SB163 Monel 400 Pipe for Chemical Industry

 

  • product-273-196
    Gnee Steel
    Wooden Boxes
  • product-273-196
    Gnee Steel
    Packing Systems
  • product-272-197
    Gnee Steel
    Wrapping Machine steel pipe
  • product-271-191
    Gnee Steel
    Fasteners Packaging

ASME SB163 Monel 400 Nickel Alloy Steel Seamless Pipe for Chemical Industry Packaging
Standard Packaging Methods:
Steel Strapping:
Pipe with an outer diameter of 3 inches or less is typically strapped together with polypropylene film to prevent rust during ocean shipping, and then secured with steel strapping.
Wooden Cases/Crates:
Pipe is typically packaged in wooden cases or crates for protection during transportation, especially long or large diameter pipe.
Seaworthy Export Packaging:
Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipe during transportation.
Typo-Proof Packaging:
Export crates are designed to prevent rain, seawater, and other external water from penetrating during transportation.

 

About Gnee Steel

Gnee Steel
About Gnee Steel

Gnee Steel is a supplier of Monel 400 Nickel-Copper Alloy. Our product offerings include seamless tubes (sizes: 4-219 mm, thicknesses: 0.5-20 mm); welded tubes (sizes: 5.0-1219.2 mm, thicknesses: 0.5-20 mm); plate (sizes: 0.1-100 mm, widths: 10-2500 mm); strip; alloy round bar (sizes: 3-800 mm, diameters: 2-100 mm, widths: 10-500 mm); hexagonal bar (sizes: 2-100 mm); wire rod; and extruded sections. We partner with steel mills to provide our customers with Alloy 400 that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS.

Gnee Steel stocks and sells Monel 400 Nickel-Copper Alloy, pipes, tubes, plates, strip, sheets, round bars, flat bars, forging billets, hexagons, wire rod, and extruded shapes. Feel free to contact us for a quote at ss@gneesteel.com

 

 

Hot Tags: ASME SB163 Monel 400 Nickel Steel Seamless Pipe For Chemical Industry, China ASME SB163 Monel 400 Nickel Steel Seamless Pipe For Chemical Industry suppliers, marine alloy, alloy disadvantage, alloy weakening, alloy knowledge, alloy revenue, flexible alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry