Alloy 713C* is a precipitation hardenable, nickel- chromium base cast alloy, which possesses excel- lent strength properties up to 1800 ºF. The alloy has good castability, remarkable resistance to oxidation and thermal fatigue, and outstanding structural stability.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 713c pipe in China. If you're going to wholesale high quality inconel alloy 713c pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 713C pipe is a special nickel-based alloy pipe that is widely regarded as a preferred material for high temperature corrosion resistance. Here are some detailed features of Inconel Alloy 713C pipe:

Corrosion resistance: Inconel 713C has good corrosion resistance to a variety of acids and bases, especially salt solutions of iron, copper, sodium, etc. It can resist corrosion from sulfur-containing gases and is particularly suitable for handling some of the harshest environments encountered in oil refining and petrochemical processes.

High temperature performance: This alloy exhibits excellent performance at high temperatures, including excellent tensile, compressive and fatigue strength, and good resistance to creep and stress rupture.

Welding performance: Inconel 713C has good weldability and can be welded by a variety of techniques, such as TIG and MIG, giving it great flexibility in construction and repair. After welding, the alloy can maintain its excellent mechanical and corrosion resistance characteristics.

Applications: Due to its corrosion resistance and high temperature resistance, Inconel 713C is often used in a variety of extreme environments such as aerospace, nuclear energy, oil and gas processing, heat treatment furnaces, heat exchangers, etc.

Standards and specifications: Inconel 713C pipe is usually manufactured in accordance with strict industrial standards, such as ASTM and ASME, to ensure the high quality and reliability of the pipe.

Forming and processing: Although Inconel 713C is difficult to process, it can be effectively formed and processed into pipes with appropriate tools and techniques to meet complex engineering requirements.

Inconel 713C Round Bar Chemical Compositons

Alloy

%

Ni

Cr

Fe

Mn

Si

Mo

Zr

Ti

Cu

Co

Al

C

S

713C

Min.

Bal

12.0

-

-

-

3.8

0.05

0.5

-

1.8

5.5

-

-

Max.

14.0

2.5

0.25

0.5

5.2

0.15

1.0

0.5

2.8

6.5

0.20

0.015

 

Inconl 713C Round Bar Physical properties

Density

7.913 g/cm³

Melting point

1260℃-1288℃

 

Inconel Alloy 713C pipeInconel Alloy 713C pipeInconel Alloy 713C pipe

Hot Tags: inconel alloy 713c pipe, China inconel alloy 713c pipe suppliers, inconel alloy seamless piping, inconel alloy vacuum forming process, 601GC Alloy Pipe, inconel alloy communication system parts, high-temperature alloy, high temperature alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry