Inconel Alloy 725 PIPE
video

Inconel Alloy 725 PIPE

Inconel 725 is a high strength nickel-based alloy. It is widely used in petrochemical, aerospace, nuclear energy and other fields. As a precipitation strengthening alloy, the mechanical properties of Inconel 725 can be improved by adjusting the heat treatment process. The precipitation strengthening properties of Inconel 725 allow it to perform well in high temperature and high stress environments. This alloy is resistant to deformation and loosening at high temperatures and is resistant to corrosion in oxidizing, reducing and mixed environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 725 pipe in China. If you're going to wholesale high quality inconel alloy 725 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 725 pipe is a type of high-performance pipe made from Inconel Alloy 725, a nickel-based superalloy. Inconel Alloy 725 is well-known for its excellent mechanical properties at high temperatures and its outstanding resistance to various forms of corrosion, including stress corrosion cracking (SCC), pitting, and oxidation.

Key Features of Inconel Alloy 725:

High-Temperature Strength: Retains strength at elevated temperatures, making it ideal for high-temperature applications.

Corrosion Resistance: Exhibits exceptional resistance to oxidation and various corrosive environments, especially in the presence of chloride ions.

Stress Corrosion Cracking Resistance: Particularly resistant to chloride stress corrosion cracking, which is a common issue in many nickel-based alloys.

Typical Mechanical Properties

Material Form and Condition Yield Strength (0.2% Offset) Tensile Strength Elongation % Hardness, Rc
ksi MPa ksi MPa
Alloy 725 round Annealed 62.0 427 124.0 855 57 5
Alloy 725 round Age Hardened 133.0 917 180.0 1241 30 36

 

Alloy 725 Chemical Composition (Wt %)

 

Carbon
(C)
Manganese
(Mn)
Phosphorus
(P)
Sulfur
(S)
Silicon
(Si)
Nickel
(Ni)
Cobalt
(Co)
0.03 Max 0.35 Max 0.015 Max 0.010 Max 0.20 Max 55.00%-59.00% -

Inconel Alloy 725 PIPEInconel Alloy 725 PIPEInconel Alloy 725 PIPE

Hot Tags: inconel alloy 725 pipe, China inconel alloy 725 pipe suppliers, inconel alloy nipple fittings, inconel alloy cooling system parts, inconel alloy terminal parts, 686 718 Inconel Pipe, inconel alloy radar system parts, metal pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry